General
Property | Value | Condition |
---|---|---|
Densidad | 2.7 g/cm³ Show Material materials with Densidad of 2.7 g/cm³ | T5 |
Mecánica
Property | Value | Condition | Comment |
---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium | |
Elongación | 2.0 % Show Material materials with Elongación of 2.0 % | T5 | |
Límite elástico | 140.0 MPa Show Material materials with Límite elástico of 140.0 MPa | T5 | |
Módulo de cizallamiento | 2.8 GPa Show Material materials with Módulo de cizallamiento of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium | |
Módulo elástico | 72.0 GPa Show Material materials with Módulo elástico of 72.0 GPa | T5 | |
Resistencia a la tracción | 170.0 MPa Show Material materials with Resistencia a la tracción of 170.0 MPa | T5 |
Aplicaciones térmicas
Property | Value | Condition |
---|---|---|
Calor específico | 970.0 J/(kg·K) Show Material materials with Calor específico of 970.0 J/(kg·K) | T5 |
Coeficiente de dilatación térmica | 2.2e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2e-05 1/K | T5 |
Conductividad térmica | 170.0 W/(m·K) Show Material materials with Conductividad térmica of 170.0 W/(m·K) | T5 |
Temperatura de fusión | 570.0 °C Show Material materials with Temperatura de fusión of 570.0 °C | T5 |
Chemical properties
Property | Value | Condition |
---|---|---|
Aluminio | 90.1 - 93.3 % Show Material materials with Aluminio of 90.1 - 93.3 % | T5 |
Cobre | 0.25 % Show Material materials with Cobre of 0.25 % | T5 |
Hierro | 0.6 % Show Material materials with Hierro of 0.6 % | T5 |
Magnesio | 0.2 - 0.45 % Show Material materials with Magnesio of 0.2 - 0.45 % | T5 |
Manganeso | 0.35 % Show Material materials with Manganeso of 0.35 % | T5 |
Otro | 0.15 % Show Material materials with Otro of 0.15 % | T5 |
Silicona | 6.5 - 7.5 % Show Material materials with Silicona of 6.5 - 7.5 % | T5 |
Titanio | 0.25 % Show Material materials with Titanio of 0.25 % | T5 |
Zinc | 0.35 % Show Material materials with Zinc of 0.35 % | T5 |