General
Property | Value | Condition |
---|---|---|
Densidad | 2.7 g/cm³ Show Material materials with Densidad of 2.7 g/cm³ | T71 |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | T71 | |||
Dureza Brinell | 60 [-] Show Material materials with Dureza Brinell of 60 [-] | T71 | 500 kg load, 10 mm b | ||
60.0 [-] Show Material materials with Dureza Brinell of 60.0 [-] | T71 | Pink Sheets, ASTM B618 | Casting | ||
70.0 [-] Show Material materials with Dureza Brinell of 70.0 [-] | T71 | Pink Sheets, ASTM B108 | Casting | ||
Elongación | 3.0 % Show Material materials with Elongación of 3.0 % | T71 | Pink Sheets, ASTM B108, ASTM B618 | Casting | A100 |
3.5 % Show Material materials with Elongación of 3.5 % | T71 | ||||
3.5 % Show Material materials with Elongación of 3.5 % | T71 | Sand cast, elongation in 50 mm | |||
Límite elástico | 125.0 MPa Show Material materials with Límite elástico of 125.0 MPa | T71 | Pink Sheets, ASTM B618 | Casting | RP02 |
140.0 MPa Show Material materials with Límite elástico of 140.0 MPa | T71 | ||||
145 MPa Show Material materials with Límite elástico of 145 MPa | T71 | Sand cast, RP02 | |||
Módulo de cizallamiento | 27.2 GPa Show Material materials with Módulo de cizallamiento of 27.2 GPa | T71 | |||
Módulo elástico | 72.0 GPa Show Material materials with Módulo elástico of 72.0 GPa | T71 | |||
72.4 GPa Show Material materials with Módulo elástico of 72.4 GPa | T71 | ||||
Resistencia a la fatiga | 59 MPa Show Material materials with Resistencia a la fatiga of 59 MPa | T71 | for 5x10⁸ cycles, R.R. Moore type test | ||
Resistencia a la tracción | 150.0 MPa Show Material materials with Resistencia a la tracción of 150.0 MPa | T71 | |||
170.0 MPa Show Material materials with Resistencia a la tracción of 170.0 MPa | T71 | Pink Sheets, ASTM B108, ASTM B618 | Casting | ||
193 MPa Show Material materials with Resistencia a la tracción of 193 MPa | T71 | Sand cast | |||
Resistencia al cizallamiento | 138 MPa Show Material materials with Resistencia al cizallamiento of 138 MPa | T71 |
Aplicaciones térmicas
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Calor específico | 970.0 J/(kg·K) Show Material materials with Calor específico of 970.0 J/(kg·K) | T71 | ||
Coeficiente de dilatación térmica | 2.2e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2e-05 1/K | T71 | ||
Conductividad térmica | 160.0 W/(m·K) Show Material materials with Conductividad térmica of 160.0 W/(m·K) | T71 | ||
Temperatura de fusión | 557.0 - 613.0 °C Show Material materials with Temperatura de fusión of 557.0 - 613.0 °C | T71 | Pink Sheets, ASTM B108, ASTM B618 | Casting |
570.0 °C Show Material materials with Temperatura de fusión of 570.0 °C | T71 |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 90.1 - 93.3 % Show Material materials with Aluminio of 90.1 - 93.3 % | T71 | ||
Cobre | 0.25 % Show Material materials with Cobre of 0.25 % | T71 | Pink Sheets, ASTM B108, ASTM B618 | Casting |
Hierro | 0.6 % Show Material materials with Hierro of 0.6 % | T71 | ||
0.60 % Show Material materials with Hierro of 0.60 % | T71 | Pink Sheets, ASTM B108, ASTM B618 | Casting | |
Magnesio | 0.2 - 0.45 % Show Material materials with Magnesio of 0.2 - 0.45 % | T71 | Pink Sheets, ASTM B108, ASTM B618 | Casting |
Manganeso | 0.35 % Show Material materials with Manganeso of 0.35 % | T71 | Pink Sheets, ASTM B108, ASTM B618 | Casting |
Otro | 0.15 % Show Material materials with Otro of 0.15 % | T71 | ||
Silicona | 6.5 - 7.5 % Show Material materials with Silicona of 6.5 - 7.5 % | T71 | Pink Sheets, ASTM B108, ASTM B618 | Casting |
Titanio | 0.25 % Show Material materials with Titanio of 0.25 % | T71 | Pink Sheets, ASTM B108, ASTM B618 | Casting |
Zinc | 0.35 % Show Material materials with Zinc of 0.35 % | T71 | Pink Sheets, ASTM B108, ASTM B618 | Casting |