General
Property | Temperature | Value |
---|---|---|
Sección transversal de captura neutrónica | 23.0 °C | 0 m² Show Supplier Material materials with Sección transversal de captura neutrónica of 0 m² |
Densidad | 23.0 °C | 10.2 g/cm³ Show Supplier Material materials with Densidad of 10.2 g/cm³ |
Masa molar | 95.94 g/mol Show Supplier Material materials with Masa molar of 95.94 g/mol |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.31 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.31 [-] | |
Dureza Vickers 10 | 23.0 °C | 160 - 180 [-] Show Supplier Material materials with Dureza Vickers 10 of 160 - 180 [-] | recrystallized |
Módulo elástico | 23.0 °C | 320 GPa Show Supplier Material materials with Módulo elástico of 320 GPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 254 J/(kg·K) Show Supplier Material materials with Calor específico of 254 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 5.2E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 5.2E-6 1/K |
Conductividad térmica | 23.0 °C | 142 W/(m·K) Show Supplier Material materials with Conductividad térmica of 142 W/(m·K) |
Punto de ebullición | 4639 °C Show Supplier Material materials with Punto de ebullición of 4639 °C | |
Temperatura de fusión | 2620 °C Show Supplier Material materials with Temperatura de fusión of 2620 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 1.79E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 1.79E+7 S/m |
Función de trabajo | 23.0 °C | 4.39 eV Show Supplier Material materials with Función de trabajo of 4.39 eV |
Resistividad eléctrica | 23.0 °C | 5.6E-8 Ω·m Show Supplier Material materials with Resistividad eléctrica of 5.6E-8 Ω·m |
Acústico
Chemical properties
Property | Value |
---|---|
Aluminio | 1E-4 % Show Supplier Material materials with Aluminio of 1E-4 % |
Cadmio | 1E-4 % Show Supplier Material materials with Cadmio of 1E-4 % |
Carbono | 1.3E-3 % Show Supplier Material materials with Carbono of 1.3E-3 % |
Cobre | 2E-4 % Show Supplier Material materials with Cobre of 2E-4 % |
Cromo | 3E-4 % Show Supplier Material materials with Cromo of 3E-4 % |
Hierro | 5E-4 % Show Supplier Material materials with Hierro of 5E-4 % |
Molibdeno | 99.97 % Show Supplier Material materials with Molibdeno of 99.97 % |
Nitrógeno | 5E-4 % Show Supplier Material materials with Nitrógeno of 5E-4 % |
Níquel | 1E-4 % Show Supplier Material materials with Níquel of 1E-4 % |
Oxígeno | 6E-4 % Show Supplier Material materials with Oxígeno of 6E-4 % |
Potasio | 6E-4 % Show Supplier Material materials with Potasio of 6E-4 % |
Silicona | 2E-4 % Show Supplier Material materials with Silicona of 2E-4 % |
Wolframio | 0.02 % Show Supplier Material materials with Wolframio of 0.02 % |
Technological properties
Property | ||
---|---|---|