General
Property | Temperature | Value | Thickness | Testing Standard | Condition | Comment |
---|---|---|---|---|---|---|
Absorción de agua | 1.5 % Show Supplier Material materials with Absorción de agua of 1.5 % | 2 mm | ISO 62 | immersion at 23°C | ||
Densidad | 1.51 g/cm³ Show Supplier Material materials with Densidad of 1.51 g/cm³ | ISO 1183 | dry | |||
Moisture absorption | 23 °C | 0.6 % Show Supplier Material materials with Moisture absorption of 0.6 % | 2 mm | ISO 62 | 50%RH |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 3 % Show Supplier Material materials with Elongación of 3 % | dry | ISO 527-2/1A | 5mm/min | |
3.2 % Show Supplier Material materials with Elongación of 3.2 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Módulo de flexión | 11.9 GPa Show Supplier Material materials with Módulo de flexión of 11.9 GPa | 50%RH | ISO 178 | 2mm/min | |
13 GPa Show Supplier Material materials with Módulo de flexión of 13 GPa | dry | ISO 178 | 2mm/min | ||
Módulo elástico | 13.4 GPa Show Supplier Material materials with Módulo elástico of 13.4 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
14.9 GPa Show Supplier Material materials with Módulo elástico of 14.9 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Resistencia a la flexión | 265 MPa Show Supplier Material materials with Resistencia a la flexión of 265 MPa | 50%RH | ISO 178 | 2mm/min | |
295 MPa Show Supplier Material materials with Resistencia a la flexión of 295 MPa | dry | ISO 178 | 2mm/min | ||
Resistencia a la tracción | 170 MPa Show Supplier Material materials with Resistencia a la tracción of 170 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
190 MPa Show Supplier Material materials with Resistencia a la tracción of 190 MPa | dry | ISO 527-2/1A | 5mm/min | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 14 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 14 kJ/m² | dry | ISO 179/1eA | |
23 °C | 15 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 15 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 17 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 17 kJ/m² | 50%RH | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | 80 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 80 kJ/m² | dry | ISO 179/1eU | -30°C | |
95 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 95 kJ/m² | dry | ISO 179/1eU | 23°C | ||
100 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 100 kJ/m² | 50%RH | ISO 179/1eU | 23°C |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 200 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 200 °C | ISO 75/2Af | 1.00E+12mm | ||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | ISO 11357-1/-3 | 10°C/min | ||
Inflamabilidad | Thickness tested (mm): 1.6, Class: HB, Standard: UL 94 | Automotive Interior Flammability(mm/min): 0 ,method: ISO 3795 and thickness tested (mm): 3 |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.2 % Show Supplier Material materials with Contracción of 0.2 % | 280/90/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
0.6 % Show Supplier Material materials with Contracción of 0.6 % | 280/90/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | Food Contact, Drinking Water, RoHS 2011/65/UE | |
Color | Black | |
Features | Hydrolysis Resistance, Heat Stabilized | |
Fillers | 50% Glass Fiber | |
Processing methods | Injection Molding |