General
Property | Temperature | Value | Condition | Testing Standard | Thickness |
---|---|---|---|---|---|
Densidad | 1.59 g/cm³ Show Supplier Material materials with Densidad of 1.59 g/cm³ | dry | ISO 1183 | ||
Moisture absorption | 23 °C | 1.2 % Show Supplier Material materials with Moisture absorption of 1.2 % | 50%RH | ISO 62 | 2 mm |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 2.4 % Show Supplier Material materials with Elongación of 2.4 % | dry | ISO 527-2/1A | 5mm/min | |
2.7 % Show Supplier Material materials with Elongación of 2.7 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Módulo de flexión | 13.4 GPa Show Supplier Material materials with Módulo de flexión of 13.4 GPa | 50%RH | ISO 178 | 2mm/min | |
15.2 GPa Show Supplier Material materials with Módulo de flexión of 15.2 GPa | dry | ISO 178 | 2mm/min | ||
Módulo elástico | 15.9 GPa Show Supplier Material materials with Módulo elástico of 15.9 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
17.9 GPa Show Supplier Material materials with Módulo elástico of 17.9 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Resistencia a la flexión | 295 MPa Show Supplier Material materials with Resistencia a la flexión of 295 MPa | 50%RH | ISO 178 | 2mm/min | |
355 MPa Show Supplier Material materials with Resistencia a la flexión of 355 MPa | dry | ISO 178 | 2mm/min | ||
Resistencia a la tracción | 190 MPa Show Supplier Material materials with Resistencia a la tracción of 190 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
240 MPa Show Supplier Material materials with Resistencia a la tracción of 240 MPa | dry | ISO 527-2/1A | 5mm/min | ||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 15.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 15.5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 16 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 16 kJ/m² | 50%RH | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | 98 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 98 kJ/m² | dry | ISO 179/1eU | 23°C | |
104 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 104 kJ/m² | 50%RH | ISO 179/1eU | 23°C |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment |
---|---|---|---|
Temperatura de fusión | 260 °C Show Supplier Material materials with Temperatura de fusión of 260 °C | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.2 % Show Supplier Material materials with Contracción of 0.2 % | 290/80/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
0.6 % Show Supplier Material materials with Contracción of 0.6 % | 290/80/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | Food Contact, RoHS 2011/65/UE | |
Color | Black | |
Features | Improved Fluiditiy, Hydrolysis Resistance, High Surface Aspect, Heat Stabilized | |
Fillers | 50% Glass Fiber | |
Processing methods | Injection Molding |