General
Property | Value | Testing Standard |
---|---|---|
Densidad | 1.2 g/cm³ Show Supplier Material materials with Densidad of 1.2 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore D | 52 [-] Show Supplier Material materials with Dureza Shore D of 52 [-] | ISO 7619-1 | 15s | |
60 [-] Show Supplier Material materials with Dureza Shore D of 60 [-] | ISO 7619-1 | inst. | ||
Elongación | 300 % Show Supplier Material materials with Elongación of 300 % | ISO 527-2/1A | 50mm/min | nominal | |
Elongation at yield | 33 % Show Supplier Material materials with Elongation at yield of 33 % | ISO 527-2/1A | 50mm/min | |
Límite elástico | 20 MPa Show Supplier Material materials with Límite elástico of 20 MPa | ISO 527-2/1A | 50mm/min | |
Modulus at 10% elongation | 0.015 GPa Show Supplier Material materials with Modulus at 10% elongation of 0.015 GPa | ISO 527-2/1A | ||
Módulo a elongación del 300 % | 0.02 GPa Show Supplier Material materials with Módulo a elongación del 300 % of 0.02 GPa | ISO 527-2/1A | ||
Módulo al 100 % de elongación | 0.018 GPa Show Supplier Material materials with Módulo al 100 % de elongación of 0.018 GPa | ISO 527-2/1A | ||
Módulo de flexión | 0.27 GPa Show Supplier Material materials with Módulo de flexión of 0.27 GPa | ISO 178 | 2mm/min | |
Módulo elástico | 0.3 GPa Show Supplier Material materials with Módulo elástico of 0.3 GPa | ISO 527-2/1A | 1mm/min | |
Resistencia a la flexión | 14 MPa Show Supplier Material materials with Resistencia a la flexión of 14 MPa | ISO 178 | 2mm/min | |
Resistencia a la tracción | 30 MPa Show Supplier Material materials with Resistencia a la tracción of 30 MPa | ISO 527-2/1A | 5mm/min | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 11 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 11 kJ/m² | ISO 179/1eA | No Break at 23°C |
Resistencia al choque, ensayo Charpy no entallado | No Break at 23°C | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment |
---|---|---|---|
Temperatura de fusión | 210 °C Show Supplier Material materials with Temperatura de fusión of 210 °C | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Velocidad de flujo de la masa derretida | 5 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 5 g/10min | ISO 1133 | 230°C/2.16Kg |
Technological properties
Property | ||
---|---|---|
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Features | Impact Modified, Heat Stabilized | |
Processing methods | Profile Extrusion,Other Extrusion |