General
Property | Temperature | Value | Thickness | Testing Standard | Condition | Comment |
---|---|---|---|---|---|---|
Absorción de agua | 7 % Show Supplier Material materials with Absorción de agua of 7 % | 2 mm | ISO 62 | immersion at 23°C | ||
Densidad | 1.35 g/cm³ Show Supplier Material materials with Densidad of 1.35 g/cm³ | ISO 1183 | dry | |||
Moisture absorption | 23 °C | 1.7 % Show Supplier Material materials with Moisture absorption of 1.7 % | 2 mm | ISO 62 | 50%RH |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 3.1 % Show Supplier Material materials with Elongación of 3.1 % | dry | ISO 527-2/1A | 5mm/min | |
Módulo de flexión | 7.8 GPa Show Supplier Material materials with Módulo de flexión of 7.8 GPa | dry | ISO 178 | 2mm/min | |
Módulo elástico | 9.4 GPa Show Supplier Material materials with Módulo elástico of 9.4 GPa | dry | ISO 527-2/1A | 1mm/min | |
Resistencia a la flexión | 245 MPa Show Supplier Material materials with Resistencia a la flexión of 245 MPa | dry | ISO 178 | 2mm/min | |
Resistencia a la tracción | 165 MPa Show Supplier Material materials with Resistencia a la tracción of 165 MPa | dry | ISO 527-2/1A | 5mm/min | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 8 kJ/m² | dry | ISO 179/1eA | |
23 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | dry | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 70 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 70 kJ/m² | dry | ISO 179/1eU | |
23 °C | 70 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 70 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Thickness | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Glow Wire Flammability Index | 700 °C Show Supplier Material materials with Glow Wire Flammability Index of 700 °C | 2 mm | IEC 60695-2-12 | ||||
Temperatura de flexión bajo carga | 215 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 215 °C | ISO 75/2Af | 1.80 MPa | ||||
235 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 235 °C | ISO 75/2Bf | 0.45 MPa | |||||
Temperatura de fusión | 245 °C Show Supplier Material materials with Temperatura de fusión of 245 °C | ISO 11357-1/-3 | 10°C/min | ||||
Temperatura de reblandecimiento Vicat | 225 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 225 °C | ISO 306 | 50°C/h 50N | ||||
Inflamabilidad | Thickness tested (mm): 0.8, Class: HB, Standard: UL 94 | Automotive Interior Flammability(mm/min): 0 ,method: ISO 3795 and thickness tested (mm): 3 |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V | |
Índice de seguimiento comparativo | 500 V Show Supplier Material materials with Índice de seguimiento comparativo of 500 V | dry | IEC 60112 | Sol.A |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.2 % Show Supplier Material materials with Contracción of 0.2 % | 280/90/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
0.7 % Show Supplier Material materials with Contracción of 0.7 % | 280/90/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Fillers | 30% Glass Fiber | |
Processing methods | Injection Molding |