General
Property | Temperature | Value | Thickness | Testing Standard | Condition | Comment |
---|---|---|---|---|---|---|
Absorción de agua | 2.5 % Show Supplier Material materials with Absorción de agua of 2.5 % | 2 mm | ISO 62 | immersion at 23°C | ||
Densidad | 1.1 g/cm³ Show Supplier Material materials with Densidad of 1.1 g/cm³ | ISO 1183 | dry | |||
Moisture absorption | 23 °C | 1.1 % Show Supplier Material materials with Moisture absorption of 1.1 % | 2 mm | ISO 62 | 50%RH |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 100 % Show Supplier Material materials with Elongación of 100 % | dry | ISO 527-2/1A | min. | 50mm/min | nominal | |
300 % Show Supplier Material materials with Elongación of 300 % | 50%RH | ISO 527-2/1A | min. | 50mm/min | nominal | ||
Elongation at yield | 55 % Show Supplier Material materials with Elongation at yield of 55 % | dry | ISO 527-2/1A | 50mm/min | |
Límite elástico | 30 MPa Show Supplier Material materials with Límite elástico of 30 MPa | 50%RH | ISO 527-2/1A | 50mm/min | |
40 MPa Show Supplier Material materials with Límite elástico of 40 MPa | dry | ISO 527-2/1A | 50mm/min | ||
Módulo de flexión | 0.62 GPa Show Supplier Material materials with Módulo de flexión of 0.62 GPa | dry | ISO 178 | 2mm/min | |
Módulo elástico | 0.53 GPa Show Supplier Material materials with Módulo elástico of 0.53 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
0.75 GPa Show Supplier Material materials with Módulo elástico of 0.75 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Resistencia a la flexión | 25 MPa Show Supplier Material materials with Resistencia a la flexión of 25 MPa | dry | ISO 178 | 2mm/min | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | dry | ISO 179/1eA | |
23 °C | 25 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 25 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 35 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 35 kJ/m² | 50%RH | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 0.00013 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.00013 1/K | ISO 11359-1/-2 | 23°C-55°C, Transverse |
0.000136 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000136 1/K | ISO 11359-1/-2 | 23°C-55°C | |
Temperatura de flexión bajo carga | 50 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 50 °C | ISO 75/2Af | 1.80 MPa |
Temperatura de fusión | 215 °C Show Supplier Material materials with Temperatura de fusión of 215 °C | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Technological properties
Property | ||
---|---|---|
Additives | Plasticizer | |
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Features | Heat Stabilized | |
Processing methods | Injection Molding,Profile Extrusion |