General
Property | Temperature | Value | Thickness | Testing Standard | Condition | Comment |
---|---|---|---|---|---|---|
Absorción de agua | 6.5 % Show Supplier Material materials with Absorción de agua of 6.5 % | 2 mm | ISO 62 | immersion at 23°C | ||
Densidad | 1.19 g/cm³ Show Supplier Material materials with Densidad of 1.19 g/cm³ | ISO 1183 | dry | |||
Moisture absorption | 23 °C | 1.9 % Show Supplier Material materials with Moisture absorption of 1.9 % | 2 mm | ISO 62 | 50%RH |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 5 % Show Supplier Material materials with Elongación of 5 % | dry | ISO 527-2/1A | 5mm/min | |
14 % Show Supplier Material materials with Elongación of 14 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Módulo de flexión | 2.2 GPa Show Supplier Material materials with Módulo de flexión of 2.2 GPa | 50%RH | ISO 178 | 2mm/min | |
4.3 GPa Show Supplier Material materials with Módulo de flexión of 4.3 GPa | dry | ISO 178 | 2mm/min | ||
Módulo elástico | 3.0 GPa Show Supplier Material materials with Módulo elástico of 3.0 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
4.8 GPa Show Supplier Material materials with Módulo elástico of 4.8 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Resistencia a la flexión | 90 MPa Show Supplier Material materials with Resistencia a la flexión of 90 MPa | 50%RH | ISO 178 | 2mm/min | |
160 MPa Show Supplier Material materials with Resistencia a la flexión of 160 MPa | dry | ISO 178 | 2mm/min | ||
Resistencia a la tracción | 65 MPa Show Supplier Material materials with Resistencia a la tracción of 65 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
102 MPa Show Supplier Material materials with Resistencia a la tracción of 102 MPa | dry | ISO 527-2/1A | 5mm/min | ||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 8 kJ/m² | dry | ISO 179/1eA | |
23 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 12 kJ/m² | 50%RH | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | 67 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 67 kJ/m² | dry | ISO 179/1eU | 23°C | |
95 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 95 kJ/m² | 50%RH | ISO 179/1eU | 23°C |
Aplicaciones térmicas
Property | Value | Thickness | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Glow Wire Flammability Index | 650 °C Show Supplier Material materials with Glow Wire Flammability Index of 650 °C | 2 mm | IEC 60695-2-12 | ||||
Temperatura de flexión bajo carga | 185 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 185 °C | ISO 75/2Af | 1.80 MPa | ||||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | ISO 11357-1/-3 | 10°C/min | ||||
Temperatura de reblandecimiento Vicat | 205 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 205 °C | ISO 306 | 1mm | ||||
Inflamabilidad | Thickness tested (mm): 0.8, Class: HB, Standard: UL 94 | Automotive Interior Flammability(mm/min): 0 ,method: ISO 3795 and thickness tested (mm): 3 |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V | |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | dry | IEC 60112 | Sol.A |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Features | Impact Modified | |
Fillers | 13% Glass Fiber | |
Processing methods | Injection Molding |