Glow Wire Flammability Index: 650 °C

Quick Comparison

Polyamide 46 (PA46)

Stanyl® TW200F6

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW241F6

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW341

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW341-FC

Suministrada por:

DSM Engineering Materials

Acrilonitrilo butadieno estireno (ABS)

Elix ABS M205FC

Suministrada por:

Elix Polymers

Polyamide 46 (PA46)

Stanyl® TW341-N

Suministrada por:

DSM Engineering Materials

Acrilonitrilo butadieno estireno (ABS)

Elix ABS P3H-AT

Suministrada por:

Elix Polymers

Acrilonitrilo butadieno estireno (ABS)

LNP™ COLORCOMP™ Compound A1000PXB

Suministrada por:

Sabic
Página 1 de 2