General
Property | Temperature | Value | Thickness | Testing Standard | Condition | Comment |
---|---|---|---|---|---|---|
Absorción de agua | 7.6 % Show Supplier Material materials with Absorción de agua of 7.6 % | 2 mm | ISO 62 | immersion at 23°C | ||
Densidad | 1.06 g/cm³ Show Supplier Material materials with Densidad of 1.06 g/cm³ | ISO 1183 | dry | |||
Moisture absorption | 23 °C | 2 % Show Supplier Material materials with Moisture absorption of 2 % | 2 mm | ISO 62 | 50%RH |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 100 % Show Supplier Material materials with Elongación of 100 % | dry, 50%RH | ISO 527-2/1A | min. | 50mm/min | nominal | |
Elongation at yield | 5 % Show Supplier Material materials with Elongation at yield of 5 % | dry | ISO 527-2/1A | 50mm/min | |
30 % Show Supplier Material materials with Elongation at yield of 30 % | 50%RH | ISO 527-2/1A | 50mm/min | ||
Límite elástico | 30 MPa Show Supplier Material materials with Límite elástico of 30 MPa | 50%RH | ISO 527-2/1A | 50mm/min | |
40 MPa Show Supplier Material materials with Límite elástico of 40 MPa | dry | ISO 527-2/1A | 50mm/min | ||
Módulo de flexión | 0.45 GPa Show Supplier Material materials with Módulo de flexión of 0.45 GPa | 50%RH | ISO 178 | 2mm/min | |
1.4 GPa Show Supplier Material materials with Módulo de flexión of 1.4 GPa | dry | ISO 178 | 2mm/min | ||
Módulo elástico | 0.6 GPa Show Supplier Material materials with Módulo elástico of 0.6 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
1.6 GPa Show Supplier Material materials with Módulo elástico of 1.6 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Resistencia a la flexión | 25 MPa Show Supplier Material materials with Resistencia a la flexión of 25 MPa | 50%RH | ISO 178 | 2mm/min | |
55 MPa Show Supplier Material materials with Resistencia a la flexión of 55 MPa | dry | ISO 178 | 2mm/min | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 25 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 25 kJ/m² | dry | ISO 179/1eA | |
23 °C | 100 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 100 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 125 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 125 kJ/m² | 50%RH | ISO 179/1eA | ||
Resistencia al choque, ensayo Izod entallado | 23 °C | 95 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 95 kJ/m² | dry | ISO 180/1A |
Aplicaciones térmicas
Property | Value | Thickness | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Glow Wire Flammability Index | 650 °C Show Supplier Material materials with Glow Wire Flammability Index of 650 °C | 2 mm | IEC 60695-2-12 | ||||
Temperatura de flexión bajo carga | 50 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 50 °C | ISO 75/2Af | 1.80 MPa | ||||
135 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 135 °C | ISO 75/2Bf | 0.45 MPa | |||||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | ISO 11357-1/-3 | 10°C/min | ||||
Temperatura de reblandecimiento Vicat | 150 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 150 °C | ISO 306 | 50°C/h 50N | ||||
Inflamabilidad | Thickness tested (mm): 0.8, Class: HB, Standard: UL 94 | Automotive Interior Flammability(mm/min): <30 ,method: ISO 3795 and thickness tested (mm): 3 |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V | |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | dry | IEC 60112 | Sol.A |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | Yellow Card, RoHS 2011/65/UE | |
Color | Natural | |
Features | Impact Modified | |
Processing methods | Injection Molding |