General
Property | Temperature | Value | Thickness | Testing Standard | Condition | Comment |
---|---|---|---|---|---|---|
Absorción de agua | 6.2 % Show Supplier Material materials with Absorción de agua of 6.2 % | 2 mm | ISO 62 | immersion at 23°C | ||
Densidad | 1.36 g/cm³ Show Supplier Material materials with Densidad of 1.36 g/cm³ | ISO 1183 | dry | |||
Moisture absorption | 23 °C | 1.6 % Show Supplier Material materials with Moisture absorption of 1.6 % | 2 mm | ISO 62 | 50%RH |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 2.7 % Show Supplier Material materials with Elongación of 2.7 % | dry | ISO 527-2/1A | 5mm/min | |
4.5 % Show Supplier Material materials with Elongación of 4.5 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Módulo de flexión | 9 GPa Show Supplier Material materials with Módulo de flexión of 9 GPa | dry | ISO 178 | 2mm/min | |
Módulo elástico | 7.3 GPa Show Supplier Material materials with Módulo elástico of 7.3 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
9.7 GPa Show Supplier Material materials with Módulo elástico of 9.7 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Resistencia a la flexión | 235 MPa Show Supplier Material materials with Resistencia a la flexión of 235 MPa | dry | ISO 178 | 2mm/min | |
Resistencia a la tracción | 105 MPa Show Supplier Material materials with Resistencia a la tracción of 105 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
148 MPa Show Supplier Material materials with Resistencia a la tracción of 148 MPa | dry | ISO 527-2/1A | 5mm/min | ||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | dry | ISO 179/1eA | |
23 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | 50%RH | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | 50 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 50 kJ/m² | dry | ISO 179/1eU | 23°C | |
65 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 65 kJ/m² | 50%RH | ISO 179/1eU | 23°C |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment |
---|---|---|---|
Temperatura de fusión | 255 °C Show Supplier Material materials with Temperatura de fusión of 255 °C | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Features | Hydrolysis Resistance, Heat Stabilized | |
Fillers | 30% Glass Fiber | |
Processing methods | Injection Molding |