General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 10.28 g/cm³ Show Supplier Material materials with Densidad of 10.28 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Módulo elástico | 23.0 °C | 329 GPa Show Supplier Material materials with Módulo elástico of 329 GPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 4.8E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 4.8E-6 1/K |
Conductividad térmica | 23.0 °C | 138 W/(m·K) Show Supplier Material materials with Conductividad térmica of 138 W/(m·K) |
Temperatura de fusión | 2623 °C Show Supplier Material materials with Temperatura de fusión of 2623 °C |
Technological properties
Property | ||
---|---|---|
Application areas | Used for processing fabricated metal products and machine parts such as wire, sheets, sintered alloys, and electronic components. Used for alloying, brake pads, ceramic metallization, diamond tooling, infiltration, and metal injection molding. Used as a chemical catalyst, detonation initiator, metal matrix composite, and sputtering target. | |
Chemical composition | Purity of ≥99.95% | |
Processing history | Molybdenum powder is produced by hydrogen reduction of molybdenum trioxide and ammonium molybdates. |