General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 11.6 g/cm³ Show Supplier Material materials with Densidad of 11.6 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Shore A | 23.0 °C | 95 [-] Show Supplier Material materials with Dureza Shore A of 95 [-] |
Elongación | 23.0 °C | 25 % Show Supplier Material materials with Elongación of 25 % |
Resistencia a desgarros | 23.0 °C | 18 kN/m Show Supplier Material materials with Resistencia a desgarros of 18 kN/m |
Resistencia a la tracción | 23.0 °C | 5.9 MPa Show Supplier Material materials with Resistencia a la tracción of 5.9 MPa |
Technological properties
Property | ||
---|---|---|
Application areas | Radiation shielding and radiation-protective equipment, X-ray inspection device for industrial and medical use, ϒ-ray shielding material and substitute for lead fiber mat in nuclear reactor piping systems. |