General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 2 - 2.19 g/cm³ Show Supplier Material materials with Densidad of 2 - 2.19 g/cm³ | For ceramic structural parts |
Tamaño de los cristales | 6 μm Show Supplier Material materials with Tamaño de los cristales of 6 μm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Módulo elástico | 23.0 °C | 235 GPa Show Supplier Material materials with Módulo elástico of 235 GPa | For ceramic structural parts |
Resistencia a la compresión | 23.0 °C | 2500 MPa Show Supplier Material materials with Resistencia a la compresión of 2500 MPa | For ceramic structural parts |
Resistencia a la flexión | 23.0 °C | 197 - 243 MPa Show Supplier Material materials with Resistencia a la flexión of 197 - 243 MPa | For ceramic structural parts |
Resistencia a la tracción | 23.0 °C | 153 MPa Show Supplier Material materials with Resistencia a la tracción of 153 MPa | For ceramic structural parts |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Conductividad térmica | 200.0 °C | 60 W/(m·K) Show Supplier Material materials with Conductividad térmica of 60 W/(m·K) | For ceramic structural parts |
900.0 °C | 43.7 W/(m·K) Show Supplier Material materials with Conductividad térmica of 43.7 W/(m·K) | For ceramic structural parts | |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 3.11E+9 Ω·m Show Supplier Material materials with Resistividad eléctrica of 3.11E+9 Ω·m | For ceramic structural parts |
Rigidez dieléctrica | 23.0 °C | 56 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 56 kV/mm | For ceramic structural parts |
Technological properties
Property | ||
---|---|---|
Application areas | Electric insulators in the vacuum system, Boron Nitride components for PVD, MOCVD, MBE system. Nozzles for nonferrous metals metallurgy industry, Spacers for glass melting, Insulators for high-temperature furnace. | |
Chemical composition | Pyrolytic Boron Nitride 99.99% | |
Processing history | Boron Nitride plates and Boron Nitride sheets are made from hot pressed boron nitride blank. Hexagonal boron nitride (H-BN) behaves similar with graphite mechanically, but offers excellent electrical resistance. |