HGFL BOPP (Biaxially Oriented Polypropylene) Transparent Film

Want to keep this datasheet? Save it now in your required format

Description

Heat-sealing transparent BOPP film with a low threshold of welding, with high coefficient of friction for a special purposes, for high quality rotogravure and flexographic printing and lamination. The main advantages are: A wide range of heat sealing; contains antistatic and antiblocking additives; excellent optical properties; good mechanical properties; intended for contact with food; high coefficient of friction stable in time; without coatings and primers.

Los datos sobre este material han sido proporcionados por Matmatch.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

Propiedades

General

PropertyTemperatureValueComment

Contracción

120.0 °C

4 - 5 %

Show Material materials with Contracción of 4 - 5 %

GOST 18616, ISO 11501, ASTM D1204 (Thermal shrinkage at 120˚C, 5 min)

Contracción transversal

120.0 °C

2 - 3 %

Show Material materials with Contracción transversal of 2 - 3 %

GOST 18616, ISO 11501, ASTM D1204 (Thermal shrinkage at 120˚C, 5 min)

Densidad

20.0 °C

0.91 g/cm³

Show Material materials with Densidad of 0.91 g/cm³

Densidad superficial

20.0 °C

1.36E-3 - 4.37E-3 g/cm²

Show Material materials with Densidad superficial of 1.36E-3 - 4.37E-3 g/cm²

Elasticidad de la película

20.0 °C

22.89 - 73.26 m²/kg

Show Material materials with Elasticidad de la película of 22.89 - 73.26 m²/kg

Medidas

PropertyValue

Espesor

0.02 - 0.05 mm

Show Material materials with Espesor of 0.02 - 0.05 mm

Dimensions

Available thicknesses: 15, 18, 20, 25, 30, 35, 40, 48µm.

Mecánica

PropertyTemperatureValueComment

Elongación

20.0 °C

200 - 220 %

Show Material materials with Elongación of 200 - 220 %

GOST 14236, ISO 527, ASTM D882

Elongación transversal

20.0 °C

70 - 80 %

Show Material materials with Elongación transversal of 70 - 80 %

GOST 14236, ISO 527, ASTM D882

Resistencia a la tracción

20.0 °C

130 - 140 MPa

Show Material materials with Resistencia a la tracción of 130 - 140 MPa

GOST 14236, ISO 527, ASTM D882

Resistencia a la tracción transversal

20.0 °C

230 - 250 MPa

Show Material materials with Resistencia a la tracción transversal of 230 - 250 MPa

GOST 14236, ISO 527, ASTM D882

Óptico

PropertyValueComment

Turbidez

2.5 - 3.2 %

Show Material materials with Turbidez of 2.5 - 3.2 %

GOST 15875, ISO 14782, ASTM D 1003

Technological properties

Property
Application areas

High quality solvent based rotogravure and flexographic printing; solvent based and solvent free lamination with polyurethane adhesives; manufacture of flexible packaging for food products; for vertical VFFS and horizontal HFFS packaging machines; laminating with PE and CPP films with a high content of slipping additives; to reduce the impact of slip additives transition from PE or CPP film to the BOPP film side, which leads to a significant coefficient of friction reduction. The high coefficient of friction of the HGFL film, provides a certain margin in this case. For a case in which the bondage process of packed products is present, for example, in pasta packaging; to save the packed packages in a single group without sliding over each other (if necessary); in the other cases, when slip reduction on BOPP side of the flexible packaging is necessary; for cold seal glue frame coating onto UT film side (if necessary).

Friction

Kinetic coefficient of friction µ= 0.4-0.65 (GOST 27492, ISO 8295, ASTM D 1894).

Other

HGFL BOPP films comprise: A treated modified heat sealable copolymer skin layer, a transparent oriented polypropylene core layer, a heat sealable, non treated skin layer with low seal intention temperature and high coefficient of friction.

Processing history

Treatment level: 38 mN/m (ISO 8296, ASTM D 2578)