General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Densidad of 7.8 g/cm³ |
Medidas
Property | Value | Comment |
---|---|---|
Ancho | 205 - 2300 mm Show Supplier Material materials with Ancho of 205 - 2300 mm | |
Espesor | 800 mm Show Supplier Material materials with Espesor of 800 mm | max. |
Longitud | 1000 - 6000 mm Show Supplier Material materials with Longitud of 1000 - 6000 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Steels |
Dureza Brinell | 23.0 °C | 156 [-] Show Supplier Material materials with Dureza Brinell of 156 [-] | |
Elongación | 23.0 °C | 28.2 % Show Supplier Material materials with Elongación of 28.2 % | |
Estricción | 23.0 °C | 55.6 % Show Supplier Material materials with Estricción of 55.6 % | |
Límite elástico | 23.0 °C | 360 MPa Show Supplier Material materials with Límite elástico of 360 MPa | |
Módulo elástico | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Módulo elástico of 200 - 210 GPa | Typical for Steels |
Resistencia a la tracción | 23.0 °C | 560 MPa Show Supplier Material materials with Resistencia a la tracción of 560 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 477 J/(kg·K) Show Supplier Material materials with Calor específico of 477 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.2E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.2E-5 1/K |
Conductividad térmica | 23.0 °C | 42.7 W/(m·K) Show Supplier Material materials with Conductividad térmica of 42.7 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 2.2E-7 Ω·m Show Supplier Material materials with Resistividad eléctrica of 2.2E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Azufre | 0.04 % Show Supplier Material materials with Azufre of 0.04 % |
Carbono | 0.28 - 0.33 % Show Supplier Material materials with Carbono of 0.28 - 0.33 % |
Cobre | 0.35 % Show Supplier Material materials with Cobre of 0.35 % |
Cromo | 0.8 - 1.1 % Show Supplier Material materials with Cromo of 0.8 - 1.1 % |
Fósforo | 0.03 % Show Supplier Material materials with Fósforo of 0.03 % |
Hierro | Balance |
Manganeso | 0.4 - 0.6 % Show Supplier Material materials with Manganeso of 0.4 - 0.6 % |
Molibdeno | 0.15 - 0.25 % Show Supplier Material materials with Molibdeno of 0.15 - 0.25 % |
Níquel | 0.25 % Show Supplier Material materials with Níquel of 0.25 % |
Silicona | 0.15 - 0.35 % Show Supplier Material materials with Silicona of 0.15 - 0.35 % |