General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Densidad of 7.8 g/cm³ |
Medidas
Property | Value | Comment |
---|---|---|
Ancho | 10 - 2500 mm Show Supplier Material materials with Ancho of 10 - 2500 mm | |
Espesor | 800 mm Show Supplier Material materials with Espesor of 800 mm | max. |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy, V-notch | 23.0 °C | 40 - 42 J Show Supplier Material materials with Charpy impact energy, V-notch of 40 - 42 J | |
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Steels |
Dureza Rockwell C | 23.0 °C | 54 - 60 [-] Show Supplier Material materials with Dureza Rockwell C of 54 - 60 [-] | |
Elongación | 23.0 °C | 10 - 12 % Show Supplier Material materials with Elongación of 10 - 12 % | |
Límite elástico | 23.0 °C | 510 - 835 MPa Show Supplier Material materials with Límite elástico of 510 - 835 MPa | |
Módulo elástico | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Módulo elástico of 200 - 210 GPa | Typical for Steels |
Resistencia a la tracción | 23.0 °C | 740 - 1270 MPa Show Supplier Material materials with Resistencia a la tracción of 740 - 1270 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.035 % Show Supplier Material materials with Azufre of 0.035 % |
Carbono | 0.38 - 0.41 % Show Supplier Material materials with Carbono of 0.38 - 0.41 % |
Cromo | 0.9 - 1.2 % Show Supplier Material materials with Cromo of 0.9 - 1.2 % |
Fósforo | 0.03 % Show Supplier Material materials with Fósforo of 0.03 % |
Hierro | Balance |
Manganeso | 0.5 - 0.8 % Show Supplier Material materials with Manganeso of 0.5 - 0.8 % |
Molibdeno | 0.15 - 0.3 % Show Supplier Material materials with Molibdeno of 0.15 - 0.3 % |
Silicona | 0.15 - 0.4 % Show Supplier Material materials with Silicona of 0.15 - 0.4 % |
Technological properties
Property | ||
---|---|---|
Application areas | Turbines,Fasteners General,Steel Bars & Rods,Burners & Boilers,Gears,Shafts,Other Valves,Bolts,Nuts,Pressure Vessels,Iron & Steel Pipes |