Medidas
Property | Value |
---|---|
Ancho | 80 - 1000 mm Show Supplier Material materials with Ancho of 80 - 1000 mm |
Diámetro | 50 - 500 mm Show Supplier Material materials with Diámetro of 50 - 500 mm |
Espesor | 20 - 400 mm Show Supplier Material materials with Espesor of 20 - 400 mm |
Longitud | 2000 - 5800 mm Show Supplier Material materials with Longitud of 2000 - 5800 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 248 [-] Show Supplier Material materials with Dureza Brinell of 248 [-] | Annealed |
Dureza Rockwell C | 23.0 °C | 60 - 62 [-] Show Supplier Material materials with Dureza Rockwell C of 60 - 62 [-] | Quenched |
Módulo elástico | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Módulo elástico of 200 - 210 GPa | Typical for Steels |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % |
Carbono | 0.95 - 1.05 % Show Supplier Material materials with Carbono of 0.95 - 1.05 % |
Cromo | 4.75 - 5.5 % Show Supplier Material materials with Cromo of 4.75 - 5.5 % |
Fósforo | 0.03 % Show Supplier Material materials with Fósforo of 0.03 % |
Hierro | Balance |
Manganeso | 1 % Show Supplier Material materials with Manganeso of 1 % |
Molibdeno | 0.9 - 1.4 % Show Supplier Material materials with Molibdeno of 0.9 - 1.4 % |
Silicona | 0.5 % Show Supplier Material materials with Silicona of 0.5 % |
Vanadio | 0.15 - 0.5 % Show Supplier Material materials with Vanadio of 0.15 - 0.5 % |