Medidas
Property | Value | Comment |
---|---|---|
Ancho | 205 - 800 mm Show Supplier Material materials with Ancho of 205 - 800 mm | |
Diámetro | 20 - 800 mm Show Supplier Material materials with Diámetro of 20 - 800 mm | |
Espesor | 800 mm Show Supplier Material materials with Espesor of 800 mm | max. |
Longitud | 300 - 5800 mm Show Supplier Material materials with Longitud of 300 - 5800 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Rockwell C | 23.0 °C | 62 - 66 [-] Show Supplier Material materials with Dureza Rockwell C of 62 - 66 [-] | Quenched |
Módulo elástico | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Módulo elástico of 200 - 210 GPa | Typical for Steels |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % |
Carbono | 0.33 - 0.43 % Show Supplier Material materials with Carbono of 0.33 - 0.43 % |
Cromo | 4.75 - 5.5 % Show Supplier Material materials with Cromo of 4.75 - 5.5 % |
Fósforo | 0.03 % Show Supplier Material materials with Fósforo of 0.03 % |
Hierro | Balance |
Manganeso | 0.2 - 0.5 % Show Supplier Material materials with Manganeso of 0.2 - 0.5 % |
Molibdeno | 1.1 - 1.6 % Show Supplier Material materials with Molibdeno of 1.1 - 1.6 % |
Níquel | 1.4 - 1.8 % Show Supplier Material materials with Níquel of 1.4 - 1.8 % |
Silicona | 0.8 - 1.2 % Show Supplier Material materials with Silicona of 0.8 - 1.2 % |
Vanadio | 0.3 - 0.6 % Show Supplier Material materials with Vanadio of 0.3 - 0.6 % |