General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Densidad of 7.8 g/cm³ |
Medidas
Property | Value | Comment |
---|---|---|
Ancho | 205 - 800 mm Show Supplier Material materials with Ancho of 205 - 800 mm | |
Diámetro | 20 - 800 mm Show Supplier Material materials with Diámetro of 20 - 800 mm | |
Espesor | 800 mm Show Supplier Material materials with Espesor of 800 mm | max. |
Longitud | 2000 - 5800 mm Show Supplier Material materials with Longitud of 2000 - 5800 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Steels |
Dureza Brinell | 23.0 °C | 217 [-] Show Supplier Material materials with Dureza Brinell of 217 [-] | |
Elongación | 23.0 °C | 12 % Show Supplier Material materials with Elongación of 12 % | |
Límite elástico | 23.0 °C | 550 MPa Show Supplier Material materials with Límite elástico of 550 MPa | |
Módulo elástico | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Módulo elástico of 200 - 210 GPa | Typical for Steels |
Resistencia a la tracción | 23.0 °C | 1080 MPa Show Supplier Material materials with Resistencia a la tracción of 1080 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.22E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.22E-5 1/K |
Conductividad térmica | 23.0 °C | 42.6 W/(m·K) Show Supplier Material materials with Conductividad térmica of 42.6 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Azufre | 0.04 % Show Supplier Material materials with Azufre of 0.04 % |
Carbono | 0.4 - 0.45 % Show Supplier Material materials with Carbono of 0.4 - 0.45 % |
Cromo | 0.8 - 1.1 % Show Supplier Material materials with Cromo of 0.8 - 1.1 % |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % |
Hierro | Balance |
Manganeso | 0.75 - 1 % Show Supplier Material materials with Manganeso of 0.75 - 1 % |
Molibdeno | 0.15 - 0.25 % Show Supplier Material materials with Molibdeno of 0.15 - 0.25 % |
Silicona | 0.15 - 0.35 % Show Supplier Material materials with Silicona of 0.15 - 0.35 % |