Medidas
Property | Value | Comment |
---|---|---|
Ancho | 205 - 800 mm Show Supplier Material materials with Ancho of 205 - 800 mm | |
Diámetro | 20 - 800 mm Show Supplier Material materials with Diámetro of 20 - 800 mm | |
Espesor | 800 mm Show Supplier Material materials with Espesor of 800 mm | max. |
Longitud | 300 - 5800 mm Show Supplier Material materials with Longitud of 300 - 5800 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 255 [-] Show Supplier Material materials with Dureza Brinell of 255 [-] | Annealed |
Dureza Rockwell C | 23.0 °C | 60 [-] Show Supplier Material materials with Dureza Rockwell C of 60 [-] | Tempered |
Módulo elástico | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Módulo elástico of 200 - 210 GPa | Typical for Steels |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % |
Carbono | 2 - 2.25 % Show Supplier Material materials with Carbono of 2 - 2.25 % |
Cromo | 11 - 12 % Show Supplier Material materials with Cromo of 11 - 12 % |
Fósforo | 0.03 % Show Supplier Material materials with Fósforo of 0.03 % |
Hierro | Balance |
Manganeso | 0.15 - 0.45 % Show Supplier Material materials with Manganeso of 0.15 - 0.45 % |
Silicona | 0.1 - 0.4 % Show Supplier Material materials with Silicona of 0.1 - 0.4 % |
Wolframio | 0.9 % Show Supplier Material materials with Wolframio of 0.9 % |