Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Dureza Rockwell C | 23.0 °C | 47 - 49 [-] Show Supplier Material materials with Dureza Rockwell C of 47 - 49 [-] | Tempered | ||
Módulo elástico | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Módulo elástico of 200 - 210 GPa | Typical for Steels | ||
Dureza Brinell | Annealed |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % |
Carbono | 0.45 % Show Supplier Material materials with Carbono of 0.45 % |
Cromo | 4.75 - 5.5 % Show Supplier Material materials with Cromo of 4.75 - 5.5 % |
Fósforo | 0.03 % Show Supplier Material materials with Fósforo of 0.03 % |
Hierro | Balance |
Manganeso | 0.2 - 0.5 % Show Supplier Material materials with Manganeso of 0.2 - 0.5 % |
Molibdeno | 1.1 - 1.75 % Show Supplier Material materials with Molibdeno of 1.1 - 1.75 % |
Silicona | 0.8 - 1.2 % Show Supplier Material materials with Silicona of 0.8 - 1.2 % |
Vanadio | 0.9 - 1.1 % Show Supplier Material materials with Vanadio of 0.9 - 1.1 % |