Medidas
Property | Value | Comment |
---|---|---|
Ancho | 205 - 800 mm Show Supplier Material materials with Ancho of 205 - 800 mm | |
Diámetro | 20 - 800 mm Show Supplier Material materials with Diámetro of 20 - 800 mm | |
Espesor | 800 mm Show Supplier Material materials with Espesor of 800 mm | max. |
Longitud | 3000 - 5800 mm Show Supplier Material materials with Longitud of 3000 - 5800 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 240 [-] Show Supplier Material materials with Dureza Brinell of 240 [-] | Annealed |
Dureza Rockwell C | 23.0 °C | 45 [-] Show Supplier Material materials with Dureza Rockwell C of 45 [-] | Hardened and Tempered |
Módulo elástico | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Módulo elástico of 200 - 210 GPa | Typical for Steels |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % |
Carbono | 0.5 - 0.6 % Show Supplier Material materials with Carbono of 0.5 - 0.6 % |
Cromo | 1 - 1.2 % Show Supplier Material materials with Cromo of 1 - 1.2 % |
Fósforo | 0.03 % Show Supplier Material materials with Fósforo of 0.03 % |
Hierro | Balance |
Manganeso | 0.65 - 0.95 % Show Supplier Material materials with Manganeso of 0.65 - 0.95 % |
Molibdeno | 0.45 - 0.55 % Show Supplier Material materials with Molibdeno of 0.45 - 0.55 % |
Níquel | 1.5 - 1.8 % Show Supplier Material materials with Níquel of 1.5 - 1.8 % |
Silicona | 0.1 - 0.4 % Show Supplier Material materials with Silicona of 0.1 - 0.4 % |
Vanadio | 0.07 - 0.12 % Show Supplier Material materials with Vanadio of 0.07 - 0.12 % |