Medidas
Property | Value |
---|---|
Diámetro | 25.4 - 355.6 mm Show Supplier Material materials with Diámetro of 25.4 - 355.6 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 388 [-] Show Supplier Material materials with Dureza Brinell of 388 [-] |
Elongación | 23.0 °C | 8 % Show Supplier Material materials with Elongación of 8 % |
Límite elástico Rp 0,2 | 23.0 °C | 1170 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 1170 MPa |
Resistencia a la tracción | 23.0 °C | 1310 MPa Show Supplier Material materials with Resistencia a la tracción of 1310 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % | ||
Carbono | 0.07 % Show Supplier Material materials with Carbono of 0.07 % | ||
Cobre | 3 - 5 % Show Supplier Material materials with Cobre of 3 - 5 % | ||
Cromo | 15 - 17.5 % Show Supplier Material materials with Cromo of 15 - 17.5 % | ||
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % | ||
Hierro | Balance | ||
Manganeso | 1 % Show Supplier Material materials with Manganeso of 1 % | ||
Níquel | 3 - 5 % Show Supplier Material materials with Níquel of 3 - 5 % | ||
Otro | 0.15 - 0.45 % Show Supplier Material materials with Otro of 0.15 - 0.45 % | Nb+Ta | |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | chemical, petrochemical, paper and general metalworking industries | |
Heat Treatment | Solution annealing at 1000 to 1050°C, hardened at 480°C | |
Welding | Good, Pre-heating and post-heating practices used for standard hardenable stainless grades are not required. Min. RREN: 17 |