Medidas
Property | Value |
---|---|
Ancho | 50 - 100 mm Show Supplier Material materials with Ancho of 50 - 100 mm |
Espesor | 5 - 10 mm Show Supplier Material materials with Espesor of 5 - 10 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy, V-notch | -46.0 °C | 45 J Show Supplier Material materials with Charpy impact energy, V-notch of 45 J | |
Dureza Brinell | 23.0 °C | 290 [-] Show Supplier Material materials with Dureza Brinell of 290 [-] | |
Elongación | 23.0 °C | 25 % Show Supplier Material materials with Elongación of 25 % | |
Límite elástico Rp 0,2 | 23.0 °C | 500 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 500 MPa | T<13MM |
Resistencia a la tracción | 23.0 °C | 630 MPa Show Supplier Material materials with Resistencia a la tracción of 630 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % |
Carbono | 0.03 % Show Supplier Material materials with Carbono of 0.03 % |
Cobre | 0.1 - 0.6 % Show Supplier Material materials with Cobre of 0.1 - 0.6 % |
Cromo | 22 - 24 % Show Supplier Material materials with Cromo of 22 - 24 % |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % |
Hierro | Balance |
Manganeso | 2 % Show Supplier Material materials with Manganeso of 2 % |
Molibdeno | 0.1 - 0.6 % Show Supplier Material materials with Molibdeno of 0.1 - 0.6 % |
Nitrógeno | 0.05 - 0.2 % Show Supplier Material materials with Nitrógeno of 0.05 - 0.2 % |
Níquel | 3.5 - 5.5 % Show Supplier Material materials with Níquel of 3.5 - 5.5 % |
Otro | B: 35 PPM |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | The main applications are for details with special requirements for high corrosion resistance. | |
Corrosion properties | Good resistance to stress corrosion cracking, Good resistance to pitting and crevice corrosion, High resistance to general corrosion, High resistance to erosion corrosion and corrosion fatigue. PREN ≥ 28 | |
Heat Treatment | Solution annealing at 1020 – 1100°C followed by water quenching | |
Welding | Very good |