Medidas
Property | Value |
---|---|
Diámetro | 3 - 650 mm Show Supplier Material materials with Diámetro of 3 - 650 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Charpy impact energy, V-notch | -195.0 °C | 60 J Show Supplier Material materials with Charpy impact energy, V-notch of 60 J |
Dureza Brinell | 23.0 °C | 215 [-] Show Supplier Material materials with Dureza Brinell of 215 [-] |
Elongación | 23.0 °C | 30 - 40 % Show Supplier Material materials with Elongación of 30 - 40 % |
Límite elástico Rp 0,2 | 23.0 °C | 205 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 205 MPa |
Resistencia a la tracción | 23.0 °C | 515 - 690 MPa Show Supplier Material materials with Resistencia a la tracción of 515 - 690 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % |
Carbono | 0.03 % Show Supplier Material materials with Carbono of 0.03 % |
Cromo | 16 - 18 % Show Supplier Material materials with Cromo of 16 - 18 % |
Fósforo | 0.45 % Show Supplier Material materials with Fósforo of 0.45 % |
Hierro | Balance |
Manganeso | 2 % Show Supplier Material materials with Manganeso of 2 % |
Molibdeno | 2 - 3 % Show Supplier Material materials with Molibdeno of 2 - 3 % |
Nitrógeno | 0.01 % Show Supplier Material materials with Nitrógeno of 0.01 % |
Níquel | 10 - 14 % Show Supplier Material materials with Níquel of 10 - 14 % |
Silicona | 0.75 % Show Supplier Material materials with Silicona of 0.75 % |
Technological properties
Property | ||
---|---|---|
Application areas | The austenitic stainless steel AISI 316L shows good acid resistance. Material AISI 316L is used in the chemical industry, apparatus engineering, sewage plants and piping industry. | |
Heat Treatment | Solution annealed and quenched in air or water. | |
Welding | Very good |