Medidas
Property | Value |
---|---|
Diámetro | 12.7 - 350 mm Show Supplier Material materials with Diámetro of 12.7 - 350 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Charpy impact energy, V-notch | -10.0 °C | 46 J Show Supplier Material materials with Charpy impact energy, V-notch of 46 J |
Dureza Rockwell C | 23.0 °C | 287 [-] Show Supplier Material materials with Dureza Rockwell C of 287 [-] |
Elongación | 23.0 °C | 25 % Show Supplier Material materials with Elongación of 25 % |
Límite elástico Rp 0,2 | 23.0 °C | 350 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 350 MPa |
Resistencia a la tracción | 23.0 °C | 770 MPa Show Supplier Material materials with Resistencia a la tracción of 770 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | |
Carbono | 0.1 % Show Supplier Material materials with Carbono of 0.1 % | |
Cobalto | 1 % Show Supplier Material materials with Cobalto of 1 % | |
Cromo | 20 - 23 % Show Supplier Material materials with Cromo of 20 - 23 % | |
Fósforo | 0.02 % Show Supplier Material materials with Fósforo of 0.02 % | |
Hierro | 5 % Show Supplier Material materials with Hierro of 5 % | |
Manganeso | 0.5 % Show Supplier Material materials with Manganeso of 0.5 % | |
Molibdeno | 8 - 10 % Show Supplier Material materials with Molibdeno of 8 - 10 % | |
Níquel | 58 % Show Supplier Material materials with Níquel of 58 % | |
Otro | 3.15 - 4.15 % Show Supplier Material materials with Otro of 3.15 - 4.15 % | Nb+Ta |
Silicona | 0.5 % Show Supplier Material materials with Silicona of 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Alloy 625 is used in oil gas industry, marine engineering, chemical processing and pollution control equipment. | |
Corrosion properties | The alloy is especially resistant to pitting and crevice corrosion but also other severely corrosive environments. | |
Heat Treatment | Solution Annealed at 890 to 1080°C. | |
Welding | Excellent |