Medidas
Property | Value |
---|---|
Diámetro | 25.4 - 230 mm Show Supplier Material materials with Diámetro of 25.4 - 230 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Charpy impact energy, V-notch | -196.0 °C | 357 J Show Supplier Material materials with Charpy impact energy, V-notch of 357 J |
Dureza Brinell | 23.0 °C | 240 [-] Show Supplier Material materials with Dureza Brinell of 240 [-] |
Elongación | 23.0 °C | 40 % Show Supplier Material materials with Elongación of 40 % |
Límite elástico Rp 0,2 | 23.0 °C | 300 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 300 MPa |
Resistencia a la tracción | 23.0 °C | 700 MPa Show Supplier Material materials with Resistencia a la tracción of 700 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % |
Carbono | 0.01 % Show Supplier Material materials with Carbono of 0.01 % |
Cobalto | 2.5 % Show Supplier Material materials with Cobalto of 2.5 % |
Cromo | 14.5 - 16.5 % Show Supplier Material materials with Cromo of 14.5 - 16.5 % |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % |
Hierro | 4 - 7 % Show Supplier Material materials with Hierro of 4 - 7 % |
Manganeso | 1 % Show Supplier Material materials with Manganeso of 1 % |
Molibdeno | 15 - 17 % Show Supplier Material materials with Molibdeno of 15 - 17 % |
Níquel | Balance |
Silicona | 0.08 % Show Supplier Material materials with Silicona of 0.08 % |
Vanadio | 0.35 % Show Supplier Material materials with Vanadio of 0.35 % |
Wolframio | 3 - 4.5 % Show Supplier Material materials with Wolframio of 3 - 4.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Usually used in chemical processing, pollution control, pulp and paper industry, waste treatment, dampers, scrubbers and heat exchangers. | |
Corrosion properties | This alloy has excellent resistance to pitting and stress corrosion cracking and oxidizing atmospheres up to 1040°C. Alloy C-276 exhibits excellent resistance in a wide variety of chemical process environments including those with ferric and cupric chlorides, hot contaminated organic and inorganic media, chlorine, formic and acetic acids, seawater, brine and hypochlorite and chlorine dioxide solutions. | |
Heat Treatment | Solution annealed at 1100 to 1160°C | |
Welding | Good |