Medidas
Property | Value |
---|---|
Diámetro | 28.1 - 82.55 mm Show Supplier Material materials with Diámetro of 28.1 - 82.55 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 250 [-] Show Supplier Material materials with Dureza Brinell of 250 [-] |
Elongación | 23.0 °C | 17 % Show Supplier Material materials with Elongación of 17 % |
Límite elástico Rp 0,2 | 23.0 °C | 620 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 620 MPa |
Resistencia a la tracción | 23.0 °C | 900 MPa Show Supplier Material materials with Resistencia a la tracción of 900 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 2.3 - 3.15 % Show Supplier Material materials with Aluminio of 2.3 - 3.15 % | ||
Azufre | 0.01 % Show Supplier Material materials with Azufre of 0.01 % | ||
Carbono | 0.25 % Show Supplier Material materials with Carbono of 0.25 % | ||
Cobre | 27 - 33 % Show Supplier Material materials with Cobre of 27 - 33 % | ||
Fósforo | 0.03 % Show Supplier Material materials with Fósforo of 0.03 % | ||
Hierro | 2 % Show Supplier Material materials with Hierro of 2 % | ||
Manganeso | 1.5 % Show Supplier Material materials with Manganeso of 1.5 % | ||
Níquel | Balance | ||
Otro | 63 % Show Supplier Material materials with Otro of 63 % | Ni+Co | |
Silicona | 0.5 % Show Supplier Material materials with Silicona of 0.5 % | ||
Titanio | 0.35 - 0.85 % Show Supplier Material materials with Titanio of 0.35 - 0.85 % |
Technological properties
Property | ||
---|---|---|
Application areas | Typical area of usage is pump shafts and oil well tools. | |
Heat Treatment | Solution annealing: 980 – 1040°C. Age hardened: 540 – 600°C. | |
Welding | Very good |