Medidas
Property | Value |
---|---|
Diámetro | 10 - 300 mm Show Supplier Material materials with Diámetro of 10 - 300 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Rockwell B | 23.0 °C | 160 [-] Show Supplier Material materials with Dureza Rockwell B of 160 [-] |
Elongación | 23.0 °C | 20 % Show Supplier Material materials with Elongación of 20 % |
Límite elástico Rp 0,2 | 23.0 °C | 276 - 448 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 276 - 448 MPa |
Resistencia a la tracción | 23.0 °C | 345 MPa Show Supplier Material materials with Resistencia a la tracción of 345 MPa |
Chemical properties
Property | Value |
---|---|
Carbono | 0.08 % Show Supplier Material materials with Carbono of 0.08 % |
Hidrógeno | 0.02 % Show Supplier Material materials with Hidrógeno of 0.02 % |
Hierro | 0.3 % Show Supplier Material materials with Hierro of 0.3 % |
Nitrógeno | 0.03 % Show Supplier Material materials with Nitrógeno of 0.03 % |
Oxígeno | 0.25 % Show Supplier Material materials with Oxígeno of 0.25 % |
Titanio | Balance |
Technological properties
Property | ||
---|---|---|
Application areas | Grade 2 titanium is also used to manufacture heat exchangers and cryogenic vessels. In seawater, Grade 2 is fully resistant to corrosion at temperatures up to 300°C. | |
Corrosion properties | It is highly resistant to chemical environments including oxidizing media, alkaline media, organic acids and compounds, aqueous salt solutions and hot gases. Its corrosion resistance holds up in liquid metals, nitric acid, mildly reducing acids and wet chlorine or bromine gas. |