Medidas
Property | Value |
---|---|
Diámetro | 6 - 255 mm Show Supplier Material materials with Diámetro of 6 - 255 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Rockwell C | 23.0 °C | 38 [-] Show Supplier Material materials with Dureza Rockwell C of 38 [-] |
Elongación | 23.0 °C | 10 - 18 % Show Supplier Material materials with Elongación of 10 - 18 % |
Límite elástico Rp 0,2 | 23.0 °C | 828 - 910 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 828 - 910 MPa |
Resistencia a la tracción | 23.0 °C | 897 - 1000 MPa Show Supplier Material materials with Resistencia a la tracción of 897 - 1000 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 5.5 - 6.8 % Show Supplier Material materials with Aluminio of 5.5 - 6.8 % |
Carbono | 0.08 % Show Supplier Material materials with Carbono of 0.08 % |
Hidrógeno | 0.02 % Show Supplier Material materials with Hidrógeno of 0.02 % |
Hierro | 0.25 % Show Supplier Material materials with Hierro of 0.25 % |
Nitrógeno | 0.05 % Show Supplier Material materials with Nitrógeno of 0.05 % |
Oxígeno | 0.2 % Show Supplier Material materials with Oxígeno of 0.2 % |
Titanio | Balance |
Vanadio | 3.5 - 4.5 % Show Supplier Material materials with Vanadio of 3.5 - 4.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | The ability to age harden this alloy makes it a good choice for such applications as springs and fasteners. | |
Welding | Grade 5 alloy is easily welded in the annealed condition, or in the solution and partially aged condition, with aging being completed during the post weld heat treatment. Precautions must be taken to prevent oxygen, nitrogen, and hydrogen contamination. Fusion welding can be done in inert gas filled chambers, or using inert gas welding of the molten metal and the adjacent heated zones using a trailing shield. Spot, seam, and flash welding can be performed without resorting to protective atmospheres. |