Medidas
Property | Value |
---|---|
Diámetro | 76.2 - 508 mm Show Supplier Material materials with Diámetro of 76.2 - 508 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Charpy impact energy, V-notch | -32.0 °C | 42 J Show Supplier Material materials with Charpy impact energy, V-notch of 42 J |
Dureza Rockwell C | 23.0 °C | 22 [-] Show Supplier Material materials with Dureza Rockwell C of 22 [-] |
Elongación | 23.0 °C | 17 - 18 % Show Supplier Material materials with Elongación of 17 - 18 % |
Límite elástico Rp 0,2 | 23.0 °C | 414 - 517 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 414 - 517 MPa |
Resistencia a la tracción | 23.0 °C | 585 - 655 MPa Show Supplier Material materials with Resistencia a la tracción of 585 - 655 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.035 % Show Supplier Material materials with Azufre of 0.035 % |
Carbono | 0.28 - 0.33 % Show Supplier Material materials with Carbono of 0.28 - 0.33 % |
Cromo | 0.8 - 1.1 % Show Supplier Material materials with Cromo of 0.8 - 1.1 % |
Fósforo | 0.03 % Show Supplier Material materials with Fósforo of 0.03 % |
Hierro | Balance |
Manganeso | 0.4 - 0.6 % Show Supplier Material materials with Manganeso of 0.4 - 0.6 % |
Molibdeno | 0.15 - 0.25 % Show Supplier Material materials with Molibdeno of 0.15 - 0.25 % |
Silicona | 0.15 - 0.35 % Show Supplier Material materials with Silicona of 0.15 - 0.35 % |
Technological properties
Property | ||
---|---|---|
Application areas | AISI 4130 is a low alloyed hardened and tempered steel used for Oil and gas drilling and production equipment – wellhead and Christmas tree equipment. | |
Heat Treatment | Hardened at 860°C followed by water quenching. Tempering at min. 650°C, cooled in air. | |
Welding | Good. |