Medidas
Property | Value |
---|---|
Diámetro | 76.2 - 254 mm Show Supplier Material materials with Diámetro of 76.2 - 254 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Charpy impact energy, V-notch | -10.0 °C | 60 J Show Supplier Material materials with Charpy impact energy, V-notch of 60 J |
Dureza Rockwell C | 23.0 °C | 27 [-] Show Supplier Material materials with Dureza Rockwell C of 27 [-] |
Elongación | 23.0 °C | 20 % Show Supplier Material materials with Elongación of 20 % |
Límite elástico Rp 0,2 | 23.0 °C | 655 - 724 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 655 - 724 MPa |
Resistencia a la tracción | 23.0 °C | 724 MPa Show Supplier Material materials with Resistencia a la tracción of 724 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 5E-3 % Show Supplier Material materials with Azufre of 5E-3 % |
Carbono | 0.03 % Show Supplier Material materials with Carbono of 0.03 % |
Cromo | 11.5 - 13.5 % Show Supplier Material materials with Cromo of 11.5 - 13.5 % |
Fósforo | 0.02 % Show Supplier Material materials with Fósforo of 0.02 % |
Hierro | Balance |
Manganeso | 1 % Show Supplier Material materials with Manganeso of 1 % |
Molibdeno | 1.5 - 2.5 % Show Supplier Material materials with Molibdeno of 1.5 - 2.5 % |
Níquel | 4.5 - 6 % Show Supplier Material materials with Níquel of 4.5 - 6 % |
Silicona | 0.5 % Show Supplier Material materials with Silicona of 0.5 % |
Titanio | 0.01 - 0.5 % Show Supplier Material materials with Titanio of 0.01 - 0.5 % |
Vanadio | 0.5 % Show Supplier Material materials with Vanadio of 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Commonly used in the same area as AISI 4130, 4140 and 4145 but often in environment, which have a high content of sulfur. | |
Heat Treatment | Hardened and tempered | |
Welding | Moderate |