Medidas
Property | Value |
---|---|
Diámetro | 152.4 - 254 mm Show Supplier Material materials with Diámetro of 152.4 - 254 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Charpy impact energy, V-notch | -10.0 °C | 20 J Show Supplier Material materials with Charpy impact energy, V-notch of 20 J |
Dureza Rockwell C | 23.0 °C | 22 [-] Show Supplier Material materials with Dureza Rockwell C of 22 [-] |
Elongación | 23.0 °C | 20 % Show Supplier Material materials with Elongación of 20 % |
Límite elástico Rp 0,2 | 23.0 °C | 550 - 655 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 550 - 655 MPa |
Resistencia a la tracción | 23.0 °C | 689 MPa Show Supplier Material materials with Resistencia a la tracción of 689 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 5E-3 % Show Supplier Material materials with Azufre of 5E-3 % |
Carbono | 0.18 - 0.22 % Show Supplier Material materials with Carbono of 0.18 - 0.22 % |
Cromo | 12.5 - 14 % Show Supplier Material materials with Cromo of 12.5 - 14 % |
Fósforo | 0.02 % Show Supplier Material materials with Fósforo of 0.02 % |
Hierro | Balance |
Manganeso | 0.25 - 1 % Show Supplier Material materials with Manganeso of 0.25 - 1 % |
Molibdeno | 0.3 % Show Supplier Material materials with Molibdeno of 0.3 % |
Níquel | 0.3 % Show Supplier Material materials with Níquel of 0.3 % |
Silicona | 0.25 - 1 % Show Supplier Material materials with Silicona of 0.25 - 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | AISI 420 Mod is a widely used in the manufacture of oil industry completion equipment such as packers, valves and pressure containing parts. Is suitable for constructional and fastener applications where moderate corrosion resistance is required. | |
Heat Treatment | Hardened and tempered | |
Welding | Moderate |