General
Property | Value |
---|---|
Densidad | 7.9 g/cm³ Show Supplier Material materials with Densidad of 7.9 g/cm³ |
Mecánica
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Coeficiente de dilatación térmica | 0.0000166 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.0000166 1/K | 20 to 200°C |
Conductividad térmica | 14 W/(m·K) Show Supplier Material materials with Conductividad térmica of 14 W/(m·K) |
Magnético
Property | Value | Comment |
---|---|---|
Permeabilidad magnética relativa | 1.01 [-] Show Supplier Material materials with Permeabilidad magnética relativa of 1.01 [-] | max. |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.01 Show Supplier Material materials with Azufre of 0.01 | max. |
Carbono | 0.08 Show Supplier Material materials with Carbono of 0.08 | max. |
Cobre | 0.25 Show Supplier Material materials with Cobre of 0.25 | max. |
Cromo | 19.5 - 22.0 % Show Supplier Material materials with Cromo of 19.5 - 22.0 % | |
Fósforo | 0.025 Show Supplier Material materials with Fósforo of 0.025 | max. |
Manganeso | 2.0 - 4.25 % Show Supplier Material materials with Manganeso of 2.0 - 4.25 % | |
Molibdeno | 2.0 - 3.0 % Show Supplier Material materials with Molibdeno of 2.0 - 3.0 % | |
Niobio | 0.25 - 0.8 % Show Supplier Material materials with Niobio of 0.25 - 0.8 % | |
Nitrógeno | 0.25 - 0.5 % Show Supplier Material materials with Nitrógeno of 0.25 - 0.5 % | |
Níquel | 9.0 - 11.0 % Show Supplier Material materials with Níquel of 9.0 - 11.0 % | |
Silicona | 0.75 Show Supplier Material materials with Silicona of 0.75 | max. |
Technological properties
Property | ||
---|---|---|
Application areas | This grade is usually used for high performance surgical implants, like thin bones screws, high mobility hip prosthesis. | |
Cold Forming | This grade has a high ability for cold drawing which means that it is possible to obtain with a wire hard drawn ( dia 8 mm max), a tensile running from 1000 MPa up to 1800 MPa depending on the requirements of the customer. |