Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 7.0 - 20.0 % Show Supplier Material materials with Elongación of 7.0 - 20.0 % | min., depending on the size |
Resistencia a la tracción | 430.0 - 780.0 MPa Show Supplier Material materials with Resistencia a la tracción of 430.0 - 780.0 MPa | depending on the size |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Transport, electronic equipment, food and food processing industry, decoration, household appliances and office systems. Machined parts, screw machining. | |
Corrosion properties | Approximately the same as for ferritic stainless steels with 17% chromium of the AISI 430 type, although its corrosion resistance is adversely affected by its high sulphur content, particularly in environments conducive to pitting or crevice corrosion. | |
Other | Available products: Other products: contact the supplier |