Chemical properties
Property | Value |
---|---|
Carbono | 0.30000000000000004 % Show Supplier Material materials with Carbono of 0.30000000000000004 % |
Cromo | 13.0 % Show Supplier Material materials with Cromo of 13.0 % |
Technological properties
Property | ||
---|---|---|
Application areas | Moulds for PVC products and glassware. Mechanical engineering, transport, electronic equipment, decoration and household appliances, cutlery: shafts, pistons, liners, valves, nuts and bolts, etc. Cutting tools. | |
Corrosion properties | Atmospheres, fresh waters (check water analysis). Oxidizing saline solutions free of chlorides, fluorides, iodides, bromides, etc. Cold diluted nitric solutions. Certain cold diluted organic acids: picric, tannic, lactic, etc. Non-corrosive products such as: alcohol, benzol, petroleum, oil and soap. | |
Heat Treatment | Tempering curves on the right side of the material page. Tempering temperature: Indicative mechanical properties after quenching in oil at 950°C and tempering for 2 hours. | |
Other | Available products: Other products: contact the supplier |