General
Property | Value |
---|---|
Densidad | 7.8 g/cm³ Show Supplier Material materials with Densidad of 7.8 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Módulo elástico | 20 °C | 200 GPa Show Supplier Material materials with Módulo elástico of 200 GPa |
100 °C | 194 GPa Show Supplier Material materials with Módulo elástico of 194 GPa | |
200 °C | 186 GPa Show Supplier Material materials with Módulo elástico of 186 GPa | |
300 °C | 180 GPa Show Supplier Material materials with Módulo elástico of 180 GPa | |
Resistencia a la tracción | 650.0 - 880.0 MPa Show Supplier Material materials with Resistencia a la tracción of 650.0 - 880.0 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20 °C | 500 J/(kg·K) Show Supplier Material materials with Calor específico of 500 J/(kg·K) | |
100 °C | 530 J/(kg·K) Show Supplier Material materials with Calor específico of 530 J/(kg·K) | ||
200 °C | 560 J/(kg·K) Show Supplier Material materials with Calor específico of 560 J/(kg·K) | ||
300 °C | 590 J/(kg·K) Show Supplier Material materials with Calor específico of 590 J/(kg·K) | ||
Coeficiente de dilatación térmica | 0.000013 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000013 1/K | 20 to 100°C | |
0.000014 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000014 1/K | 20 to 300°C | ||
0.000135 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000135 1/K | 20 to 200°C | ||
Conductividad térmica | 20 °C | 15 W/(m·K) Show Supplier Material materials with Conductividad térmica of 15 W/(m·K) | |
100 °C | 16 W/(m·K) Show Supplier Material materials with Conductividad térmica of 16 W/(m·K) | ||
200 °C | 17 W/(m·K) Show Supplier Material materials with Conductividad térmica of 17 W/(m·K) | ||
300 °C | 18 W/(m·K) Show Supplier Material materials with Conductividad térmica of 18 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20 °C | 0.0000008 Ω·m Show Supplier Material materials with Resistividad eléctrica of 0.0000008 Ω·m |
100 °C | 0.00000085 Ω·m Show Supplier Material materials with Resistividad eléctrica of 0.00000085 Ω·m | |
200 °C | 0.0000009 Ω·m Show Supplier Material materials with Resistividad eléctrica of 0.0000009 Ω·m | |
300 °C | 0.000001 Ω·m Show Supplier Material materials with Resistividad eléctrica of 0.000001 Ω·m |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.015 Show Supplier Material materials with Azufre of 0.015 | max. |
Carbono | 0.03 Show Supplier Material materials with Carbono of 0.03 | max. |
Cobre | 0.1 - 0.6000000000000001 % Show Supplier Material materials with Cobre of 0.1 - 0.6000000000000001 % | |
Cromo | 22.0 - 24.0 % Show Supplier Material materials with Cromo of 22.0 - 24.0 % | |
Fósforo | 0.035 Show Supplier Material materials with Fósforo of 0.035 | max. |
Manganeso | 2.0 Show Supplier Material materials with Manganeso of 2.0 | max. |
Molibdeno | 0.1 - 0.6000000000000001 % Show Supplier Material materials with Molibdeno of 0.1 - 0.6000000000000001 % | |
Nitrógeno | 0.05 - 0.2 % Show Supplier Material materials with Nitrógeno of 0.05 - 0.2 % | |
Níquel | 3.5 - 5.5 % Show Supplier Material materials with Níquel of 3.5 - 5.5 % | |
Silicona | 1.0 Show Supplier Material materials with Silicona of 1.0 | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Hydraulic and pneumatic mechanisms | |
Corrosion properties | As UGICHROM® is "stainless in mass" there are no corrosion resistance problems over time, provided that the chosen grade is appropriate to the place of use. Passive layer: Stainless steels produce a very fine surface film of oxide consisting of chromium oxides and hydroxides a few Angströms thick. This oxide, commonly called a passive layer, protects the stainless steel against external attacks and gives it the property known as inoxidibility which guarantees the corrosion resistance of these alloys. The passive layer is an intrinsic part of the material, unlike the "Nickel-Chromium" coating deposited on carbon steels, which explains why stainless steel exhibits the basic corrosion resistance and adhesion advantages of chromium under harsh mechanical operating conditions (buckling). Once formed, this passive layer is completely stable since its thickness remains constant. The passive layer inhibits any exchange between the metal and the outside: in the event of damage to the material (scratch, cut, impact, drilling, deformation, etc.), it reforms spontaneously. This self-restructuring is also called "Repassivation". Choosing the most suitable grade: Only choosing the grade that is most appropriate to the operating environment increases the durability of hydraulic cylinders, depending on use. The figure on the right side of the material page shows how to obtain the best compromise between mechanical strength and corrosion resistance (see the chart on the right side of the material page). | |
Other | The mechanical properties of UGICHROM® are suitable for all hydraulic applications: Conditioning: The UGICHROM® product range offers a wide variety of conditioning options suitable for all customers' needs: Individual protection: Possibility of continuous ink jet marking on individual extruded plastic protection. Packaging: |