General
Property | Value |
---|---|
Densidad | 7.9 g/cm³ Show Supplier Material materials with Densidad of 7.9 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 25.0 - 30.0 % Show Supplier Material materials with Elongación of 25.0 - 30.0 % | min., depending on the size | |
Módulo elástico | 20 °C | 200 GPa Show Supplier Material materials with Módulo elástico of 200 GPa | |
100 °C | 194 GPa Show Supplier Material materials with Módulo elástico of 194 GPa | ||
200 °C | 186 GPa Show Supplier Material materials with Módulo elástico of 186 GPa | ||
300 °C | 180 GPa Show Supplier Material materials with Módulo elástico of 180 GPa | ||
400 °C | 172 GPa Show Supplier Material materials with Módulo elástico of 172 GPa | ||
500 °C | 165 GPa Show Supplier Material materials with Módulo elástico of 165 GPa | ||
Resistencia a la tracción | 500.0 - 950.0 MPa Show Supplier Material materials with Resistencia a la tracción of 500.0 - 950.0 MPa | min., depending on the size |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 500 J/(kg·K) Show Supplier Material materials with Calor específico of 500 J/(kg·K) | |
Coeficiente de dilatación térmica | 0.000016 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000016 1/K | 20 to 100°C |
0.0000165 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.0000165 1/K | 20 to 200°C | |
0.000017 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000017 1/K | 20 to 300°C | |
0.0000175 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.0000175 1/K | 20 to 400°C | |
0.000018 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000018 1/K | 20 to 500°C | |
Conductividad térmica | 15 W/(m·K) Show Supplier Material materials with Conductividad térmica of 15 W/(m·K) |
Eléctrico
Property | Value |
---|---|
Resistividad eléctrica | 7.3e-07 Ω·m Show Supplier Material materials with Resistividad eléctrica of 7.3e-07 Ω·m |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.03 Show Supplier Material materials with Azufre of 0.03 | max. |
Carbono | 0.08 Show Supplier Material materials with Carbono of 0.08 | max. |
Cromo | 17.0 - 19.0 % Show Supplier Material materials with Cromo of 17.0 - 19.0 % | |
Fósforo | 0.045 Show Supplier Material materials with Fósforo of 0.045 | max. |
Manganeso | 2.0 Show Supplier Material materials with Manganeso of 2.0 | max. |
Molibdeno | 0.5 Show Supplier Material materials with Molibdeno of 0.5 | max. |
Níquel | 9.0 - 12.0 % Show Supplier Material materials with Níquel of 9.0 - 12.0 % | |
Silicona | 1.0 Show Supplier Material materials with Silicona of 1.0 | max. |
Titanio | 0.7000000000000001 Show Supplier Material materials with Titanio of 0.7000000000000001 | max., min: 5x(C+N) |
Technological properties
Property | ||
---|---|---|
Application areas | ||
Corrosion properties | It has excellent corrosion resistance in natural environments (drinkable water, rural and urban environments) and in food processing and agri-food environments (but with reservations in some specific cases, such as white wines, mustards, etc.). | |
General machinability | Turning: Not only does UGIMA® 4541 reduce tool wear (see the graph on the right for improvements in terms of potential turning productivity), it also provides better chip breakability (see graph on the right for the number of cutting conditions with fragmented chips in turning). | |
Heat Treatment | Annealing: UGIMA® 4541 heat treatment involves maintaining a high temperature of between 1000°C and 1100°C, followed by air- or water-cooling. This treatment, which is called annealing, removes all trace of hardening, while giving the steel its lowest level of mechanical properties. | |
Hot forming | UGIMA® 4541 can be forged at between 950°C and 1250°C without taking special precautions. As for all austenitic stainless steel grades, the force required to deform metals is high (far higher than that required for carbon steels). Components can be air- or water-cooled. | |
Other | Available products: Other options: contact the supplier | |
Surface Treatment | The conditions generally used for austenitic grades apply to UGIMA® 4541. | |
Welding | UGIMA® 4541 can be welded by all types of arc processes (MIG, TIG with or without filler metal, coated electrodes, submerged arc welding, etc.), resistance (spot or seam), friction, electron beam or LASER welding. |