General
Property | Value | Comment |
---|---|---|
Espesor de la capa | 3.5 Show Supplier Material materials with Espesor de la capa of 3.5 | |
Número de capa | 1.0 - 10.0 [-] Show Supplier Material materials with Número de capa of 1.0 - 10.0 [-] | ≤5 is 60%, ≤10 is 90% and >10 is 10%, using Raman |
Tamaño de lámina lateral | 10000.0 Show Supplier Material materials with Tamaño de lámina lateral of 10000.0 | Using SEM |
Mecánica
Property | Value |
---|---|
Módulo elástico | 1000.0 GPa Show Supplier Material materials with Módulo elástico of 1000.0 GPa |
Resistencia a la tracción | 13000.0 MPa Show Supplier Material materials with Resistencia a la tracción of 13000.0 MPa |
Aplicaciones térmicas
Property | Value |
---|---|
Conductividad térmica | 5000 W/(m·K) Show Supplier Material materials with Conductividad térmica of 5000 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Azufre | 1.0 % Show Supplier Material materials with Azufre of 1.0 % |
Carbono | 97.0 - 99.0 % Show Supplier Material materials with Carbono of 97.0 - 99.0 % |
Flúor | 1.0 % Show Supplier Material materials with Flúor of 1.0 % |
Nitrógeno | 0.6000000000000001 % Show Supplier Material materials with Nitrógeno of 0.6000000000000001 % |
Oxígeno | 1.0 - 3.0 % Show Supplier Material materials with Oxígeno of 1.0 - 3.0 % |
Technological properties
Property | ||
---|---|---|
Application areas | Being electrically conductive, thermally conductive and a highly effective mechanical reinforcer there are numerous potential applications for graphene such as: composites, energy, biomedical, membranes, coatings, sensors, electronics |