General
Property | Value | Comment |
---|---|---|
Número de capa | 1.0 - 100.0 [-] Show Supplier Material materials with Número de capa of 1.0 - 100.0 [-] | Using AFM |
Tamaño de lámina lateral | 20000.0 Show Supplier Material materials with Tamaño de lámina lateral of 20000.0 | Using SEM/AFM |
Chemical properties
Property | Value |
---|---|
Azufre | 3.0 % Show Supplier Material materials with Azufre of 3.0 % |
Carbono | 87.5 - 92.5 % Show Supplier Material materials with Carbono of 87.5 - 92.5 % |
Manganeso | 3.0 % Show Supplier Material materials with Manganeso of 3.0 % |
Nitrógeno | 5.0 % Show Supplier Material materials with Nitrógeno of 5.0 % |
Oxígeno | 4.5 - 19.5 % Show Supplier Material materials with Oxígeno of 4.5 - 19.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | li-ion batteries, fuel cells, battery electrodes, solar pv cells, electrically conductive inks, thermally conductive films and coatings, thermal interface materials, lightweight composites, concrete, metal -matrix composites, corrosion protection, barrier properties / permeation / mechanical performance. | |
Color | Black |