General
Property | Value |
---|---|
Espesor de la capa | 0.005 - 0.015 µm Show Supplier Material materials with Espesor de la capa of 0.005 - 0.015 µm |
Tamaño de lámina lateral | 500.0 - 1500.0 nm Show Supplier Material materials with Tamaño de lámina lateral of 500.0 - 1500.0 nm |
Eléctrico
Property | Value | Comment |
---|---|---|
Surface resistivity | 10.0 Ω/sq Show Supplier Material materials with Surface resistivity of 10.0 Ω/sq | For 25µm thickness |
Rheological Properties
Property | Value |
---|---|
Viscosidad | 0.6000000000000001 Pa·s Show Supplier Material materials with Viscosidad of 0.6000000000000001 Pa·s |
Technological properties
Property | ||
---|---|---|
Application areas | flexible electronics | |
Processing methods | Flexo, Gravure, Screen Printing, Blade, Meyer Bar Coating - with a drying condition of 100℃ for 10 min |