General
Property | Value | Comment |
---|---|---|
Número de capa | 1.0 - 100.0 [-] Show Supplier Material materials with Número de capa of 1.0 - 100.0 [-] | ≤5 is 18%, ≤10 is 73% and 10-100 is 27%, using Raman |
Tamaño de lámina lateral | 26500.0 Show Supplier Material materials with Tamaño de lámina lateral of 26500.0 | Using SEM |
Chemical properties
Property | Value |
---|---|
Azufre | 2.0 % Show Supplier Material materials with Azufre of 2.0 % |
Carbono | 93.0 - 99.0 % Show Supplier Material materials with Carbono of 93.0 - 99.0 % |
Flúor | 2.0 % Show Supplier Material materials with Flúor of 2.0 % |
Nitrógeno | 0.6000000000000001 % Show Supplier Material materials with Nitrógeno of 0.6000000000000001 % |
Oxígeno | 1.0 - 5.0 % Show Supplier Material materials with Oxígeno of 1.0 - 5.0 % |
Technological properties
Property | ||
---|---|---|
Application areas | Being electrically conductive, thermally conductive and a highly effective mechanical reinforcer there are numerous potential applications for graphene such as: composites, energy, biomedical, membranes, coatings, sensors, electronics |