General
Property | Value | Comment |
---|---|---|
Número de capa | 1.0 - 2.0 [-] Show Supplier Material materials with Número de capa of 1.0 - 2.0 [-] | Predominantly few-layer with some mono-layer and bi-layer |
Tamaño de lámina lateral | 5000.0 Show Supplier Material materials with Tamaño de lámina lateral of 5000.0 | Using SEM |
Mecánica
Property | Value |
---|---|
Módulo elástico | 1000.0 GPa Show Supplier Material materials with Módulo elástico of 1000.0 GPa |
Aplicaciones térmicas
Property | Value |
---|---|
Conductividad térmica | 1700 W/(m·K) Show Supplier Material materials with Conductividad térmica of 1700 W/(m·K) |
2000 W/(m·K) Show Supplier Material materials with Conductividad térmica of 2000 W/(m·K) |
Eléctrico
Property | Value |
---|---|
Banda prohibida | 6.0 eV Show Supplier Material materials with Banda prohibida of 6.0 eV |
Chemical properties
Property | Value |
---|---|
Boro | 40.0 - 44.0 % Show Supplier Material materials with Boro of 40.0 - 44.0 % |
Carbono | 6.0 - 10.0 % Show Supplier Material materials with Carbono of 6.0 - 10.0 % |
Nitrógeno | 43.0 - 47.0 % Show Supplier Material materials with Nitrógeno of 43.0 - 47.0 % |
Oxígeno | 2.0 - 4.0 % Show Supplier Material materials with Oxígeno of 2.0 - 4.0 % |
Technological properties
Property | ||
---|---|---|
Application areas | The lamellar structure of h-BN offers exceptional benefits as an additive in lubricants, and the high thermal conductivity and electrically insulating properties have promoted its use as a high performance additive for specialist lubricants, particularly where heat removal and electrical insulation are paramount. h-BN can be included in ceramics, alloys, resins, plastics and rubbers to improve insulating ability. Electronics, oxygen sensors, xerographic processes and laser printing. Proton conductors, fuel cells, water electrolysis. Thermofluids and thermal management |