General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Densidad | 20.0 °C | 2.73 g/cm³ Show Material materials with Densidad of 2.73 g/cm³ | H15 | EN 573-3 | Tube |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | H15 | EN 573-3 | Tube | |
Dureza Brinell | 20.0 °C | 44.0 [-] Show Material materials with Dureza Brinell of 44.0 [-] | H15 | EN 573-3 | Tube | |
Elongación | 20.0 °C | 4.0 % Show Material materials with Elongación of 4.0 % | H15 | EN 573-3 | Tube | A50 |
20.0 °C | 5.0 % Show Material materials with Elongación of 5.0 % | H15 | EN 573-3 | Tube | ||
Módulo de cizallamiento | 20.0 °C | 24.0 - 26.5 GPa Show Material materials with Módulo de cizallamiento of 24.0 - 26.5 GPa | H15 | EN 573-3 | Tube | |
20.0 °C | 24.0 - 26.1 GPa Show Material materials with Módulo de cizallamiento of 24.0 - 26.1 GPa | H15 | EN 573-3 | Tube | ||
20.0 °C | 26.1 - 26.5 GPa Show Material materials with Módulo de cizallamiento of 26.1 - 26.5 GPa | H15 | EN 573-3 | Tube | ||
20.0 °C | 26.1 GPa Show Material materials with Módulo de cizallamiento of 26.1 GPa | H15 | EN 573-3 | Tube | ||
Módulo elástico | -270.0 °C | 70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | H15 | EN 573-3 | Tube | |
20.0 °C | 69.0 - 70.0 GPa Show Material materials with Módulo elástico of 69.0 - 70.0 GPa | H15 | EN 573-3 | Tube | ||
20.0 °C | 69.0 - 69.5 GPa Show Material materials with Módulo elástico of 69.0 - 69.5 GPa | H15 | EN 573-3 | Tube | ||
20.0 °C | 69.0 GPa Show Material materials with Módulo elástico of 69.0 GPa | H15 | EN 573-3 | Tube | ||
20.0 °C | 69.5 - 70.0 GPa Show Material materials with Módulo elástico of 69.5 - 70.0 GPa | H15 | EN 573-3 | Tube | ||
20.0 °C | 69.5 GPa Show Material materials with Módulo elástico of 69.5 GPa | H15 | EN 573-3 | Tube | ||
20.0 °C | 70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | H15 | EN 573-3 | Tube | ||
50.0 °C | 69.0 GPa Show Material materials with Módulo elástico of 69.0 GPa | H15 | EN 573-3 | Tube | ||
100.0 °C | 68.0 GPa Show Material materials with Módulo elástico of 68.0 GPa | H15 | EN 573-3 | Tube | ||
150.0 °C | 66.0 GPa Show Material materials with Módulo elástico of 66.0 GPa | H15 | EN 573-3 | Tube | ||
200.0 °C | 63.0 GPa Show Material materials with Módulo elástico of 63.0 GPa | H15 | EN 573-3 | Tube | ||
250.0 °C | 57.0 GPa Show Material materials with Módulo elástico of 57.0 GPa | H15 | EN 573-3 | Tube | ||
300.0 °C | 50.0 GPa Show Material materials with Módulo elástico of 50.0 GPa | H15 | EN 573-3 | Tube | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 3000 Series Aluminium | ||||
Resistencia a la tracción | 20.0 °C | 145.0 - 180.0 MPa Show Material materials with Resistencia a la tracción of 145.0 - 180.0 MPa | H15 | EN 573-3 | Tube |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 20.0 °C | 892.0 - 893.0 J/(kg·K) Show Material materials with Calor específico of 892.0 - 893.0 J/(kg·K) | H15 | EN 573-3 | Tube | |
20.0 °C | 892.0 J/(kg·K) Show Material materials with Calor específico of 892.0 J/(kg·K) | H15 | EN 573-3 | Tube | ||
20.0 °C | 893.0 J/(kg·K) Show Material materials with Calor específico of 893.0 J/(kg·K) | H15 | EN 573-3 | Tube | ||
Coeficiente de dilatación térmica | 2.2e-05 - 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2e-05 - 2.4e-05 1/K | Typical for Wrought 3000 Series Aluminium | ||||
Conductividad térmica | 20.0 °C | 160.0 - 200.0 W/(m·K) Show Material materials with Conductividad térmica of 160.0 - 200.0 W/(m·K) | H15 | EN 573-3 | Tube | |
20.0 °C | 160.0 W/(m·K) Show Material materials with Conductividad térmica of 160.0 W/(m·K) | H15 | EN 573-3 | Tube | ||
Temperatura de fusión | 629.0 - 654.0 °C Show Material materials with Temperatura de fusión of 629.0 - 654.0 °C | Typical for Wrought 3000 Series Aluminium |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Conductividad eléctrica | 20.0 °C | 22000000.0 - 28000000.0 S/m Show Material materials with Conductividad eléctrica of 22000000.0 - 28000000.0 S/m | H15 | EN 573-3 | Tube |
20.0 °C | 22000000.0 - 29000000.0 S/m Show Material materials with Conductividad eléctrica of 22000000.0 - 29000000.0 S/m | H15 | EN 573-3 | Tube | |
Resistividad eléctrica | 20.0 °C | 3.4e-08 - 4.1e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.4e-08 - 4.1e-08 Ω·m | H15 | EN 573-3 | Tube |
20.0 °C | 3.4e-08 - 4.5e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.4e-08 - 4.5e-08 Ω·m | H15 | EN 573-3 | Tube | |
20.0 °C | 4.1e-08 Ω·m Show Material materials with Resistividad eléctrica of 4.1e-08 Ω·m | H15 | EN 573-3 | Tube | |
20.0 °C | 4.1e-08 - 4.5e-08 Ω·m Show Material materials with Resistividad eléctrica of 4.1e-08 - 4.5e-08 Ω·m | H15 | EN 573-3 | Tube |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.1 Show Material materials with Cobre of 0.1 | H15 | EN 573-3 | Tube |
Cromo | 0.1 Show Material materials with Cromo of 0.1 | H15 | EN 573-3 | Tube |
Hierro | 0.7 Show Material materials with Hierro of 0.7 | H15 | EN 573-3 | Tube |
Magnesio | 0.3 Show Material materials with Magnesio of 0.3 | H15 | EN 573-3 | Tube |
Manganeso | 0.9 - 1.5 % Show Material materials with Manganeso of 0.9 - 1.5 % | H15 | EN 573-3 | Tube |
Silicona | 0.5 Show Material materials with Silicona of 0.5 | H15 | EN 573-3 | Tube |
Zinc | 0.2 Show Material materials with Zinc of 0.2 | H15 | EN 573-3 | Tube |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |