General
Property | Value | Comment |
---|---|---|
Densidad | 2.75 - 2.84 g/cm³ Show Material materials with Densidad of 2.75 - 2.84 g/cm³ | Typical for Wrought 2000 Series Aluminium |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 2000 Series Aluminium | ||||
Dureza Brinell | 20.0 °C | 125.0 [-] Show Material materials with Dureza Brinell of 125.0 [-] | T652 | WL 3.1924-1 | Forging | Transverse |
20.0 °C | 125.0 [-] Show Material materials with Dureza Brinell of 125.0 [-] | T652 | WL 3.1924-1 | Forging | ||
Módulo de cizallamiento | 26.0 - 27.5 GPa Show Material materials with Módulo de cizallamiento of 26.0 - 27.5 GPa | Typical for Wrought 2000 Series Aluminium | ||||
Módulo elástico | 70.0 - 73.0 GPa Show Material materials with Módulo elástico of 70.0 - 73.0 GPa | Typical for Wrought 2000 Series Aluminium | ||||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 2000 Series Aluminium | ||||
Resistencia a la tracción | 20.0 °C | 380.0 MPa Show Material materials with Resistencia a la tracción of 380.0 MPa | T652 | WL 3.1924-1 | Forging | Transverse |
20.0 °C | 390.0 MPa Show Material materials with Resistencia a la tracción of 390.0 MPa | T652 | WL 3.1924-1 | Forging | Transverse | |
20.0 °C | 400.0 MPa Show Material materials with Resistencia a la tracción of 400.0 MPa | T652 | WL 3.1924-1 | Forging | ||
20.0 °C | 410.0 MPa Show Material materials with Resistencia a la tracción of 410.0 MPa | T652 | WL 3.1924-1 | Forging | Transverse | |
20.0 °C | 420.0 MPa Show Material materials with Resistencia a la tracción of 420.0 MPa | T652 | WL 3.1924-1 | Forging |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 816.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 816.0 - 963.0 J/(kg·K) | Typical for Wrought 2000 Series Aluminium |
Coeficiente de dilatación térmica | 1.6e-05 - 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6e-05 - 2.4e-05 1/K | Typical for Wrought 2000 Series Aluminium |
Conductividad térmica | 112.0 - 251.0 W/(m·K) Show Material materials with Conductividad térmica of 112.0 - 251.0 W/(m·K) | Typical for Wrought 2000 Series Aluminium |
Temperatura de fusión | 500.0 - 650.0 °C Show Material materials with Temperatura de fusión of 500.0 - 650.0 °C | Typical for Wrought 2000 Series Aluminium |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 18000000.0 - 30000000.0 S/m Show Material materials with Conductividad eléctrica of 18000000.0 - 30000000.0 S/m | Typical for Wrought 2000 Series Aluminium |
Resistividad eléctrica | 3.4e-08 - 6e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.4e-08 - 6e-08 Ω·m | Typical for Wrought 2000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 1.8 - 2.7 % Show Material materials with Cobre of 1.8 - 2.7 % | T652 | WL 3.1924-1 | Forging |
Hierro | 0.9 - 1.4 % Show Material materials with Hierro of 0.9 - 1.4 % | T652 | WL 3.1924-1 | Forging |
Magnesio | 1.2 - 1.8 % Show Material materials with Magnesio of 1.2 - 1.8 % | T652 | WL 3.1924-1 | Forging |
Manganeso | 0.2 Show Material materials with Manganeso of 0.2 | T652 | WL 3.1924-1 | Forging |
Níquel | 0.8 - 1.4 % Show Material materials with Níquel of 0.8 - 1.4 % | T652 | WL 3.1924-1 | Forging |
Silicona | 0.15 - 0.25 % Show Material materials with Silicona of 0.15 - 0.25 % | T652 | WL 3.1924-1 | Forging |
Titanio | 0.2 Show Material materials with Titanio of 0.2 | T652 | WL 3.1924-1 | Forging |
Zinc | 0.1 Show Material materials with Zinc of 0.1 | T652 | WL 3.1924-1 | Forging |
Technological properties
Property | ||
---|---|---|
Workability | Moderate Workability |