General
Property | Value | Comment |
---|---|---|
Densidad | 2.65 - 2.71 g/cm³ Show Material materials with Densidad of 2.65 - 2.71 g/cm³ | Typical for Cast 4xx.x Series Aluminium |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Bending Fatigue Strength | 60.0 - 90.0 MPa Show Material materials with Bending Fatigue Strength of 60.0 - 90.0 MPa | F | EN 1706 | Casting | |
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 4xx.x Series Aluminium | |||
Dureza Brinell | 60.0 [-] Show Material materials with Dureza Brinell of 60.0 [-] | F | EN 1706 | Casting | |
Módulo elástico | 71.0 - 75.0 GPa Show Material materials with Módulo elástico of 71.0 - 75.0 GPa | Typical for Cast 4xx.x Series Aluminium | |||
Resistencia a la tracción | 240.0 MPa Show Material materials with Resistencia a la tracción of 240.0 MPa | F | EN 1706 | Casting |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 963.0 J/(kg·K) Show Material materials with Calor específico of 963.0 J/(kg·K) | Typical for Cast 4xx.x Series Aluminium | ||||
Coeficiente de dilatación térmica | 20 °C | 1.9999999999999998e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.9999999999999998e-05 1/K | F | EN 1706 | Casting | |
100 °C | 1.9999999999999998e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.9999999999999998e-05 1/K | F | EN 1706 | Casting | ||
Conductividad térmica | 130.0 - 160.0 W/(m·K) Show Material materials with Conductividad térmica of 130.0 - 160.0 W/(m·K) | F | EN 1706 | Casting | ||
Temperatura de fusión | 565.0 - 630.0 °C Show Material materials with Temperatura de fusión of 565.0 - 630.0 °C | Typical for Cast 4xx.x Series Aluminium |
Eléctrico
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Conductividad eléctrica | 16000000.0 - 22000000.0 S/m Show Material materials with Conductividad eléctrica of 16000000.0 - 22000000.0 S/m | F | EN 1706 | Casting |
Resistividad eléctrica | 4.54e-08 - 6.25e-08 Ω·m Show Material materials with Resistividad eléctrica of 4.54e-08 - 6.25e-08 Ω·m | F | EN 1706 | Casting |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 83.65 % Show Material materials with Aluminio of 83.65 % | F | EN 1706 | |
Cobre | 0.2 % Show Material materials with Cobre of 0.2 % | F | EN 1706 | Casting |
Hierro | 1.0 % Show Material materials with Hierro of 1.0 % | F | EN 1706 | |
1.0 % Show Material materials with Hierro of 1.0 % | F | EN 1706 | Casting | |
Magnesio | 0.4 % Show Material materials with Magnesio of 0.4 % | F | EN 1706 | Casting |
Manganeso | 0.55 % Show Material materials with Manganeso of 0.55 % | F | EN 1706 | Casting |
Silicona | 10.0 - 13.5 % Show Material materials with Silicona of 10.0 - 13.5 % | F | EN 1706 | Casting |
Titanio | 0.15 % Show Material materials with Titanio of 0.15 % | F | EN 1706 | Casting |
Zinc | 0.3 % Show Material materials with Zinc of 0.3 % | F | EN 1706 | Casting |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: not recommended | |
Corrosion properties | general: not sufficient | |
General machinability | as cast: acceptable | |
Processing methods | pressure die casting, separately cast test sample |