General
Property | Value |
---|---|
Densidad relativa | 8.8 [-] Show Supplier Material materials with Densidad relativa of 8.8 [-] |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Vickers | 197 [-] Show Supplier Material materials with Dureza Vickers of 197 [-] | H Temper |
229 [-] Show Supplier Material materials with Dureza Vickers of 229 [-] | EH Temper | |
242 [-] Show Supplier Material materials with Dureza Vickers of 242 [-] | SH Temper | |
258 [-] Show Supplier Material materials with Dureza Vickers of 258 [-] | ESH Temper | |
285 [-] Show Supplier Material materials with Dureza Vickers of 285 [-] | XSH Temper | |
Elongación | 2.1 % Show Supplier Material materials with Elongación of 2.1 % | XSH Temper |
9.3 % Show Supplier Material materials with Elongación of 9.3 % | ESH Temper | |
13.3 % Show Supplier Material materials with Elongación of 13.3 % | SH Temper | |
23.2 % Show Supplier Material materials with Elongación of 23.2 % | EH Temper | |
35.3 % Show Supplier Material materials with Elongación of 35.3 % | H Temper | |
Límite elástico | 469 MPa Show Supplier Material materials with Límite elástico of 469 MPa | H Temper | for spring material (Kb0.1) |
563 MPa Show Supplier Material materials with Límite elástico of 563 MPa | EH Temper | for spring material (Kb0.1) | |
569 MPa Show Supplier Material materials with Límite elástico of 569 MPa | H Temper, RP02 | |
632 MPa Show Supplier Material materials with Límite elástico of 632 MPa | SH Temper | for spring material (Kb0.1) | |
648 MPa Show Supplier Material materials with Límite elástico of 648 MPa | ESH Temper | for spring material (Kb0.1) | |
694 MPa Show Supplier Material materials with Límite elástico of 694 MPa | EH Temper, RP02 | |
706 MPa Show Supplier Material materials with Límite elástico of 706 MPa | XSH Temper | for spring material (Kb0.1) | |
773 MPa Show Supplier Material materials with Límite elástico of 773 MPa | SH Temper, RP02 | |
834 MPa Show Supplier Material materials with Límite elástico of 834 MPa | ESH Temper, RP02 | |
968 MPa Show Supplier Material materials with Límite elástico of 968 MPa | XSH Temper, RP02 | |
Módulo de flexión | 100 GPa Show Supplier Material materials with Módulo de flexión of 100 GPa | |
Módulo elástico | 110 GPa Show Supplier Material materials with Módulo elástico of 110 GPa | |
Plegabilidad 90 ° bidireccional | 0 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 0 [-] | H Temper |
0 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 0 [-] | EH Temper | |
0 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 0 [-] | SH Temper | |
2 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 2 [-] | ESH Temper | |
4 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 4 [-] | XSH Temper | |
Plegabilidad 90 ° en peso bruto | 0 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 0 [-] | H Temper |
0 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 0 [-] | EH Temper | |
0 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 0 [-] | SH Temper | |
0 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 0 [-] | ESH Temper | |
0 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 0 [-] | XSH Temper | |
Resistencia a la tracción | 616 MPa Show Supplier Material materials with Resistencia a la tracción of 616 MPa | H Temper |
721 MPa Show Supplier Material materials with Resistencia a la tracción of 721 MPa | EH Temper | |
778 MPa Show Supplier Material materials with Resistencia a la tracción of 778 MPa | SH Temper | |
845 MPa Show Supplier Material materials with Resistencia a la tracción of 845 MPa | ESH Temper | |
979 MPa Show Supplier Material materials with Resistencia a la tracción of 979 MPa | XSH Temper |
Aplicaciones térmicas
Property | Value |
---|---|
Calor específico | 377 J/(kg·K) Show Supplier Material materials with Calor específico of 377 J/(kg·K) |
Coeficiente de dilatación térmica | 1.82e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.82e-05 1/K |
Conductividad térmica | 63 W/(m·K) Show Supplier Material materials with Conductividad térmica of 63 W/(m·K) |
Temperatura de fusión | 880 - 1020 °C Show Supplier Material materials with Temperatura de fusión of 880 - 1020 °C |
Eléctrico
Property | Value |
---|---|
Specific Electrical conductivity | 12 % IACS Show Supplier Material materials with Specific Electrical conductivity of 12 % IACS |
Chemical properties
Property | Value | Comment |
---|---|---|
Estaño | 7 - 9 % Show Supplier Material materials with Estaño of 7 - 9 % | |
Fósforo | 0.03 - 0.2 % Show Supplier Material materials with Fósforo of 0.03 - 0.2 % | |
Hierro | 0.01 % Show Supplier Material materials with Hierro of 0.01 % | max. |
Otro | 99.8 % Show Supplier Material materials with Otro of 99.8 % | min. | Cu+Sn+P |
Plomo | 0.01 % Show Supplier Material materials with Plomo of 0.01 % | max. |
Zinc | 0.01 % Show Supplier Material materials with Zinc of 0.01 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | The grade is particularly suitable for electronics (connectors, lead frames, lead terminals, transistor terminals, etc.), electrical (relay and switch contacts, rotary switch slides and contacts, fuse clips, etc.), automotive (bearing frames, hydraulic equipment caps, packing, bearings, clutch disks, electrical parts, etc.) and others (bellows, slides, blades, plate springs, corrosion-proof machinery equipment, diaphragms, etc.) | |
Coating | Standard product specification of a HOT-DIP-tinned strip. *Width means the slit width after plating. *Different plating thickness for each side is possible. * We can accommodate our products to individual specifications other than the above standard specifications. Please feel free to call us. | |
Other | Please contact the supplier if you have any specific requests regarding chemical compostions, mechanical properties, and thickness. | |
Tolerances |