General
Property | Value |
---|---|
Densidad relativa | 8.82 [-] Show Supplier Material materials with Densidad relativa of 8.82 [-] |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Vickers | 203 [-] Show Supplier Material materials with Dureza Vickers of 203 [-] | H Temper |
214 [-] Show Supplier Material materials with Dureza Vickers of 214 [-] | EH Temper | |
222 [-] Show Supplier Material materials with Dureza Vickers of 222 [-] | SH Temper | |
Elongación | 12.7 % Show Supplier Material materials with Elongación of 12.7 % | SH Temper |
13.7 % Show Supplier Material materials with Elongación of 13.7 % | EH Temper | |
22.6 % Show Supplier Material materials with Elongación of 22.6 % | H Temper | |
Límite elástico | 614 MPa Show Supplier Material materials with Límite elástico of 614 MPa | H Temper | RP02 |
697 MPa Show Supplier Material materials with Límite elástico of 697 MPa | EH Temper | RP02 | |
739 MPa Show Supplier Material materials with Límite elástico of 739 MPa | SH Temper | RP02 | |
Módulo de flexión | 105 GPa Show Supplier Material materials with Módulo de flexión of 105 GPa | |
Módulo elástico | 115 GPa Show Supplier Material materials with Módulo elástico of 115 GPa | |
Plegabilidad 90 ° bidireccional | 0 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 0 [-] | H Temper |
0 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 0 [-] | EH Temper | |
1 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 1 [-] | SH Temper | |
Plegabilidad 90 ° en peso bruto | 0 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 0 [-] | H Temper |
0 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 0 [-] | EH Temper | |
1 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 1 [-] | SH Temper | |
Resistencia a la tracción | 630 MPa Show Supplier Material materials with Resistencia a la tracción of 630 MPa | H Temper |
699 MPa Show Supplier Material materials with Resistencia a la tracción of 699 MPa | EH Temper | |
744 MPa Show Supplier Material materials with Resistencia a la tracción of 744 MPa | SH Temper |
Aplicaciones térmicas
Property | Value |
---|---|
Calor específico | 375 J/(kg·K) Show Supplier Material materials with Calor específico of 375 J/(kg·K) |
Coeficiente de dilatación térmica | 1.82e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.82e-05 1/K |
Conductividad térmica | 67 W/(m·K) Show Supplier Material materials with Conductividad térmica of 67 W/(m·K) |
Temperatura de fusión | 900 - 1040 °C Show Supplier Material materials with Temperatura de fusión of 900 - 1040 °C |
Eléctrico
Property | Value |
---|---|
Specific Electrical conductivity | 14 % IACS Show Supplier Material materials with Specific Electrical conductivity of 14 % IACS |
Chemical properties
Property | Value | Comment |
---|---|---|
Estaño | 5.5 - 7 % Show Supplier Material materials with Estaño of 5.5 - 7 % | |
Fósforo | 0.03 - 0.2 % Show Supplier Material materials with Fósforo of 0.03 - 0.2 % | |
Hierro | 0.01 % Show Supplier Material materials with Hierro of 0.01 % | max. |
Otro | 99.8 % Show Supplier Material materials with Otro of 99.8 % | min. | Cu+Sn+P |
Plomo | 0.01 % Show Supplier Material materials with Plomo of 0.01 % | max. |
Zinc | 0.01 % Show Supplier Material materials with Zinc of 0.01 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | The grade is particularly suitable for electronics (connectors, lead frames, lead terminals, transistor terminals, etc.), electrical (relay and switch contacts, rotary switch slides and contacts, fuse clips, etc.), automotive (bearing frames, hydraulic equipment caps, packing, bearings, clutch disks, electrical parts, etc.) and others (bellows, slides, blades, plate springs, corrosion-proof machinery equipment, diaphragms, etc.) | |
Coating | Standard product specification of a HOT-DIP-tinned strip. *Width means the slit width after plating. *Different plating thickness for each side is possible. * We can accommodate our products to individual specifications other than the above standard specifications. Please feel free to call us. | |
Other | Please contact the supplier if you have any specific requests regarding chemical compostions, mechanical properties, and thickness. | |
Tolerances |